Next Article in Journal
Green, Black and Rooibos Tea Inhibit Prostaglandin E2 Formation in Human Monocytes by Inhibiting Expression of Enzymes in the Prostaglandin E2 Pathway
Next Article in Special Issue
Microwave Synthesis of Copper Phyllosilicates as Effective Catalysts for Hydrogenation of C≡C Bonds
Previous Article in Journal
Preparation of Hollow Core–Shell Fe3O4/Nitrogen-Doped Carbon Nanocomposites for Lithium-Ion Batteries
Previous Article in Special Issue
Noble Metal Nanoparticles Stabilized by Hyper-Cross-Linked Polystyrene as Effective Catalysts in Hydrogenation of Arenes
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

Nitrous Oxide Adsorption and Decomposition on Zeolites and Zeolite-like Materials

by
Leonid M. Kustov
1,2,3,*,
Sergey F. Dunaev
1,2,3 and
Alexander L. Kustov
1,2,3
1
Chemistry Department, Moscow State University, 1 Leninskie Gory, Bldg. 3, 119991 Moscow, Russia
2
N.D. Zelinsky Institute of Organic Chemistry RAS, 47 Leninsky Prosp., 119991 Moscow, Russia
3
Institute of Ecotechnologies and Engineering, National University of Science and Technology MISiS, 4 Leninsky Prosp., 119049 Moscow, Russia
*
Author to whom correspondence should be addressed.
Submission received: 18 December 2021 / Revised: 31 December 2021 / Accepted: 6 January 2022 / Published: 8 January 2022
(This article belongs to the Special Issue Catalysis by Hybrid Materials)

Abstract

:
Decomposition of N2O on modified zeolites, crystalline titanosilicalites, and related amorphous systems is studied by the catalytic and spectroscopic methods. Zinc-containing HZSM-5 zeolites and titanosilicalites with moderate Ti/Si ratios are shown to exhibit a better catalytic performance in N2O decomposition as compared with conventionally used Cu/HZSM-5 zeolites and amorphous Cu-containing catalysts. Dehydroxylation of the HZSM-5 zeolite by calcination at 1120 K results in an enhancement of the N2O conversion. The mechanism of the reaction and the role of coordinatively unsaturated cations and Lewis acid sites in N2O decomposition are discussed on the basis of the spectroscopic data.

1. Introduction

The problem of N2O decomposition remains to gradually attract attention in view of the development of green technologies. This problem is related to the synthesis of adipic acid, which yields N2O as a side product, as well as NOx abatement in exhaust gases of power plants or waste anesthetic gas purification. Furthermore, the reaction of N2O decomposition was shown to be the initial and key stage in the processes of selective oxidation of aromatic compounds with N2O under mild conditions using zeolites as catalysts [1,2,3,4,5,6]. It was shown that coordinatively unsaturated cations (iron species and framework Lewis acid sites) are responsible for the catalytic activity of dehydroxylated HZSM-5 zeolites both in N2O decomposition and in the reactions of oxidation of various aromatic substrates using N2O [3,4,5]. In the art, oxide systems are known as N2O decomposition catalysts, with amorphous copper oxide, for instance, Cu-Me/Al2O3, as well as cobalt oxide systems [7], magnesium cobaltite MgxCo1−xCo2O4 [8], CoOx-CeO2 [9] or Co-Ce spinel [10] as quite active, although most of the Co-based catalysts, except for the Co-Ce spinel, demonstrate high conversion only at high temperatures (870–1070 K). Ceria-zirconia behaves nearly similar to Co-oxide materials [11].
Other supported catalysts, such as rhodium on lanthanum silicate Rh/La10Si6−xFexO27−δ or Pt/ZrO2 providing a 100% N2O conversion at temperatures as high as 870 K [12,13] or Pt, Ir, and Pd supported on Al2O3 [14] have been also studied. However, the use of noble metals seems to be an expensive way to N2O abatement. Furthermore, carbon nanotubes were predicted by DFT calculations to catalyze this reaction [15].
Among the most efficient catalysts used for N2O decomposition, high-silica zeolites modified with iron [5,16], rhodium [17], copper [18], ruthenium [19], and mixed Co-In [20] ions were shown to demonstrate the best performance. The reported catalysts provide a complete conversion of nitrous oxide to nitrogen and oxygen at 620 K. Ru(0) nanoclusters prepared by the reduction of Ru(III) ions, as well as osmium(III) species were found to be less active compared with ruthenium ions. The systems containing Fe, Cu, Co, and Ru metal ions exhibited a much better catalytic performance in N2O decomposition as compared with other modified and non-modified zeolites [21], as well as other amorphous oxide systems [22,23]. The main disadvantages revealed, for example, by the Cu-catalysts for N2O decomposition are their low thermal stability (they irreversibly lose the activity after overheating to T > 870 K) and poor tolerance to admixtures of H2O, CO, CO2, and hydrocarbons, which are present in real gas mixtures and act as poisons. The behavior of catalysts definitely depends on the presence of water vapor in the feed, as well as other residual components (NO, O2, NO2) that may interfere with the N2O decomposition process [24]. However, in the mixture, we will limit our scope with the model conditions, without the introduction of other potentially important ingredients.
The aim of this work was to find new zeolite and zeolite-like catalysts that are active in N2O decomposition and to study the nature of active sites and plausible reaction mechanisms, with an emphasis on the role of coordinatively unsaturated cations. Three groups of catalysts were chosen for the investigation:
Dehydroxylated HZSM-5 zeolites and ZSM-5 zeolites modified with zinc oxide, which have been studied earlier from the point of view of the nature and strength of Lewis acid sites [25,26], i.e., the systems containing strong coordinatively unsaturated cations (Lewis acid sites);
Crystalline Ti-silicalites that are widely used as efficient catalysts for the selective oxidation of phenol into diphenols by H2O2 in the liquid phase [27];
Amorphous catalysts, based on the Ti/SiO2 system, which differ in the Ti/Si ratio and in the preparation method.
For comparative purposes, the well-known Cu-ZSM-5-type catalysts for N2O decomposition, as well as amorphous Cu-containing oxide systems were also studied.

2. Results and Discussion

To evaluate the relative strength of coordinatively unsaturated cations in the modified zeolites under study and to rank the samples according to the relative concentration of strong electron-acceptor centers, IR spectra of molecular hydrogen, as a probe for low-coordinated cations [28], were measured.
Figure 1 shows the IR spectra of H2 adsorbed at 77 K on three representative samples containing rather strong coordinatively unsaturated cations: (1) Dehydroxylated HZSM-5 zeolite, (2) Cu/HZSM-5, and (3) Zn/HZSM-5. The absorption bands in the region of 4100–4120 cm−1 correspond to weakly bonded H2 complexes with bridging Si(OH)Al and terminal SiOH groups, respectively [28], whereas the bands below 4100 cm−1 are shown [28] to belong to complexes of molecular hydrogen with coordinatively unsaturated cations (or Lewis acid sites) that exhibit electron-accepting properties. The stronger the interaction in the complex, i.e., the stronger the electron-acceptor center, the larger the shift of the corresponding band of adsorbed H2 toward lower frequencies measured relative to the frequency of the H-H stretching vibration in the gas phase (νH-H = 4163 cm−1) [28]. As seen from the spectra shown in Figure 1, the strongest coordinatively unsaturated cations are present in the Zn/ZSM-5 zeolite (νH-H = 3955, 4010 and 4070 cm−1, for these bands ΔνH-H = 208, 153, and 93 cm−1, respectively), whereas the weakest centers among the three catalysts under consideration are revealed in the dehydroxylated HZSM-5 zeolite (νH-H = 4010 and 4035 cm−1, ΔνH-H = 153 and 128 cm−1, respectively). The Cu/ZSM-5 zeolite, which is the well-known active catalyst for N2O decomposition, manifests an intermediate strength of the electron-acceptor centers (νH-H = 3970 and 4060 cm−1, ΔνH-H = 193 and 103 cm−1, respectively). Of note, the concentration of the strongest electron-acceptor centers is the highest for the Zn/HZSM-5 zeolite. Moreover, it is noteworthy that a further increase in the loading of copper in the Cu/HZSM-5 zeolite from 1 to 3 wt%, as well as an increase in the loading of zinc in the Zn/HZSM-5 zeolite over 5 wt%, have no appreciable effect on the spectral pattern, i.e., the concentration of strong Lewis acid sites. Furthermore, this increase does not improve the catalytic performance of the Cu-zeolite and Zn-zeolite catalysts.
The pre-adsorption of a small amount of N2O at 300 K on the zeolite samples, which precedes the adsorption of H2 results in the disappearance of the low-frequency absorption bands attributed to the H2 complexes with low-coordinated cations. However, this has no considerable influence on the intensity of the high-frequency bands (νH-H = 4100–4120 cm−1) assigned to the complexes with OH groups. This experiment shows that adsorption of N2O occurs on the low-coordinated metal cations that are responsible for the appearance of the corresponding absorption bands in the IR spectra of adsorbed hydrogen.
The adsorption of N2O on the zeolite samples results in the appearance of the absorption bands at 2285–2230 cm−1 (Figure 2). The frequency of gaseous N2O is 2224 cm−1. Herein, we observe one band at 2230 cm−1, which is close to the gas-phase value (physically adsorbed N2O) and a shifted band at 2285 cm−1 due to complexes with zinc species (electron-acceptor centers). The largest shift of the N2O band with respect to the corresponding band position for N2O molecules in the gas phase is observed for Zn/HZSM-5 zeolites (ν = 2285 cm−1, Δν = 50 cm−1), which indicates the strongest polarization and activation of the N2O molecule by the electron-acceptor sites of the Zn/HZSM-5 zeolite. According to our previous spectroscopic data and quantum-chemical calculation [1,2], the N2O molecule is preferably adsorbed on the Lewis acid center (for instance, on trigonally coordinated aluminum ions) by a two-point mechanism, which also involves a neighboring oxygen atom of the surface cluster. In this case, adsorption of N2O is accompanied by a considerable change of the geometry of the molecule, in particular, by a substantial decrease of the NNO angle (from 180 to 140°) and by a strong polarization of the N-O bond, which favors the further decomposition of the N2O molecule with the evolution of N2 into the gas phase and chemisorption of atomic oxygen [1,2]. Evidently, the extent of N2O polarization and activation, and thus, the rate of decomposition are governed by the strength of coordinatively unsaturated cations. Correspondingly, heating of the Zn/HZSM-5 zeolite with pre-adsorbed N2O at 520 K for 1 h directly in the IR cell (under static conditions) leads to the complete decomposition of N2O, and the bands at 2285–2240 cm−1 vanish from the spectrum, whereas the corresponding band at 2355 cm−1 appears due to the molecular nitrogen formed upon the N2O decomposition. For comparison, heating of the dehydroxylated HZSM-5 zeolite with pre-adsorbed N2O at 520 K for 1 h results only in a partial decomposition of N2O, in accordance with a weaker strength of the low-coordinated cations (Lewis acid sites).
To reveal subtle distinctions in the properties of the modified zeolites related to N2O decomposition, we tested the samples in the flow catalytic unit at 620–900 K. The reaction conditions and the conversion degrees for the N2O decomposition on the modified HZSM-5 zeolites and some Cu-containing amorphous catalysts used for NOx decomposition are summarized in Table 1. In agreement with the spectroscopic data, the dehydroxylated HZSM-5 zeolite exhibits a poor conversion even at enhanced temperatures (720 K), and the Zn-containing zeolites reveal the best performance. These catalysts are active at low temperatures as 620 K (the conversion of 85%), while the known Cu/HZSM-5 system exhibits a considerable inferior performance (the conversion does not exceed 20%) under the same conditions. Of note, both samples of the amorphous Cu-containing catalysts show a poor performance as compared with the Zn- and Cu-zeolites. The presence of low-coordinated metal ions (zinc or copper) should clearly be considered as the pre-requisite for the efficient N2O decomposition. Therefore, the spectroscopic and catalytic data indicate that strong electron-acceptor (low-coordinated) metal ions, which should actually be considered as Lewis acid-base pair sites containing a low-coordinated metal ion and an oxygen anion of the framework, are presumably the active centers responsible for the N2O decomposition on the modified zeolites. With the analogy from our previous studies and taking into account the results of quantum-chemical calculations [1,2], we may propose the following mechanism of N2O decomposition on strong coordinatively unsaturated metal ions, which involves strong perturbation of the N2O molecule and further formation of the chemisorbed oxygen atom. Here, the latter is consumed for the recombination or scavenged by the second N2O molecule, yielding N2 and O2 (Scheme 1):
The second group of catalysts studied in the reaction of N2O decomposition comprised crystalline Ti-silicalites with different Si/Ti ratios and amorphous TiO2-SiO2 systems. The Ti-silicalites have been chosen for the investigation in the title reaction, since they exhibit unique catalytic properties in the reactions of selective oxidation of phenol into diphenols using H2O2 as an oxidizing agent [27,29]. The active centers responsible for these properties of the Ti-silicalites are should be titanyl groups Ti=O or isolated tetrahedral Ti+4 ions [29]. Accordingly, the reaction is assumed to involve Ti-OOH fragments in the coordination sphere of the isolated Ti+4 ions. Taking into account the fact that the N2O molecule contains labile oxygen, similar to the H2O2 molecule, and with due regard to the similarity of the reaction mechanisms for the selective oxidation with N2O and H2O2, which include activation and decomposition of the molecule of the oxidizing agent, we may assume that the catalysts which are active in the reactions involving H2O2, i.e., Ti-silicalites, will be active in the reaction of N2O decomposition.
Table 2 presents the results of catalytic testing of various Ti systems in the reaction of N2O decomposition. The N2O conversion for the crystalline Ti-silicalites of the TS-1 type (four samples) passes through a maximum at Si/Ti = 32. Of note, the performance of the crystalline Ti-silicalite with the Si/Ti ratio equal to 32 is higher than the known Cu/HZSM-5 catalyst, especially at low temperatures (620–645 K). The dome-shaped dependence of the N2O decomposition rate for the Ti-silicalites versus the Si/Ti ratio may be accounted for in the following way. Evidently, a decrease in the performance with the increasing Si/Ti ratio from 32 to 38 results from a diminution of the concentration of active isolated Ti+4 ions in the framework. A decrease in the conversion degree when the Ti content in the samples increases (the Si/Ti ratio decreases to 20–15), may be equally explained by a decrease in the concentration of the active isolated Ti+4 species as a result of the growth of the concentration of the pair Ti+4 centers, which are likely inactive (or less active, as compared with the isolated Ti+4 species). The concentration of the isolated Ti+4 species may also decrease due to the formation of octahedral Ti+4 centers, in particular, extra-framework octahedral species, for instance, in the form of anatase, which is inactive in the N2O decomposition, at least in the temperature range studied. The latter hypothesis is consistent with the data presented by Bellussi et al. [30], who showed that the probability of the formation of anatase (or in general, octahedral Ti+4 ions) during the synthesis of Ti-silicalites of the TS-1 type drastically increases, when the Si/Ti ratio approaches 20 and lower values.
For a comparison with the crystalline Ti-silicalites, we also tested the performance of amorphous TiO2-SiO2 samples. Here, it is known [31] that the amorphous Ti/SiO2 is completely inactive in the reaction of selective oxidation of phenol with aqueous solutions of H2O2. Moreover, these samples exhibited a very low conversion in the reaction of N2O decomposition. Furthermore, they revealed some N2O conversion only at high temperatures of 720–770 K, while the crystalline Ti-silicalites with a close Si/Ti ratio were very active at 620 K.
To ascertain the coordination state of titanium ions in the crystalline and amorphous Ti-systems, we used the XPS method. Figure 3 depicts the representative XP spectra of two crystalline samples and one amorphous catalyst. The spectra contain a characteristic line of Ti 3p3/2 in the range of the binding energies of 460.0–458.7 eV. For the Ti-silicalite with a moderate Si/Ti ratio (32), a sharp peak at 460.0 eV is observed, which is ascribed to tetrahedrally coordinated Ti+4 ions, whereas for Ti-silicalites with lower Si/Ti ratios (22.9 and 14.4), a superposition of the peak at 460.0 eV with the second line with the maximum at 458.7 eV is revealed as a result of the presence of octahedrally coordinated Ti+4 ions. A similar spectral pattern is observed for the amorphous TiO2-SiO2 sample.
With an analogy regarding the chemistry of processes based on H2O2, one may consider two plausible reaction mechanisms for N2O decomposition on the Ti-silicalites (Scheme 2):
The first mechanism is similar to the one proposed for the modified zeolites contain-ing coordinatively unsaturated cations, such as Zn/HZSM-5, except for the fact that Ti+4 ions are not in the trigonal but in the tetragonal coordination. However, taking into account the fact that (1) for Ti+4 ions the characteristic coordination numbers are 4 and 6, and (2) tetragonal Ti+4 ions in the framework of Ti-silicalites are capable of coordinating additional adsorbate molecules, we may consider the first mechanism as one of the possible ways of N2O transformation. The aforementioned XPS data lend some support for this mechanism of N2O decomposition. However, of note, the presence of five-coordinated titanium ions cannot be excluded, since the XPS pattern represents a superposition of at least two, maybe three lines. The five-coordinated titanium ions are also coordinatively unsaturated and therefore, can take part in the reaction. The second mechanism involves a cyclic peroxo complex, which also seems quite probable in view of the data obtained for the so-called “reactive silica” [32]. In any case, discrimination between these two mechanisms should be done in the future research, probably, with the help of labelled isotopes of oxygen.
Figure 4 displays the IR spectra of two samples of the crystalline Ti-silicalites measured after N2O adsorption at room temperature and after heating the sample with pre-adsorbed N2O at 520 K directly in the IR cell under static conditions. Unlike Zn/HZSM-5 zeolites, the adsorption of N2O does not result in a considerable polarization and perturbation of the molecule, and the band position for adsorbed N2O (ΔνH-H = 2235–2225 cm−1) is very close to the physically adsorbed N2O. Nevertheless, heating of the samples at 570 K for 1 h results in the complete (the sample with Si/A = 32) or considerable (the sample with Si/Al = 14.4) disappearance of the N2O absorption bands. Simultaneously, the bands of N2 at 2360–2340 cm−1 are formed, thereby indicating the decomposition of N2O. These data agree fairly well with the catalytic data presented in Table 2.

3. Materials and Methods

The dehydroxylated HZSM-5 zeolite was prepared by calcination of the HZSM-5 zeolite (Si/Al = 20) in a vacuum at 1120 K for 2 h. Zn/HZSM-5 catalysts with ZnO loadings of 1–5 wt% were synthesized by wet impregnation of the HZSM-5 zeolite with a 1 M aqueous solution of Zn(NO3)2, with further drying at 390 K in air and successive calcination in air at 820 K for 4 h and 920 K for 4 h. Four samples of crystalline Ti-silicalites of the TS-1 type with Si/Ti ratios of 14.4, 22.9, 32.0, and 37.9 were prepared according to the known procedure [30]. The Cu/HZSM-5 zeolite with 3 wt% Cu, which corresponded to the maximum conversion on the zeolite in N2O decomposition, was prepared by wet impregnation of the HZSM-5 zeolite similar to the Zn/HZSM-5 samples. The crystallinity of the zeolites and Ti-silicalites under study, monitored by XRD, was close to 95–100%.
Samples of amorphous Ti/SiO2 catalysts were prepared by the method of chemical vapor deposition (CVD) using TiCl4 and the sample of silica gel with successive hydrolysis or by coprecipitation of TiO2 and SiO2. The resulting Ti/SiO2 catalysts were characterized by TiO2 loadings of 0.5–80 wt%. The Co-Cr-Cu/Al2O3 catalyst for N2O decomposition was prepared by the co-precipitation of equimolar amounts of Co, Cr, and Cu from their nitrate precursors, in the presence of γ-Al2O3 (surface area, 170 m2/g) with further calcination at 770 K for 2 h.
In this paper, the structure of all the studied zeolite samples, including the starting HZSM-5, dehydroxylated HZSM-5, Zn/HZSM-5, Cu/HZSM-5, and TS-1 samples with any Si/Ti ratio, present the same MFI type, as determined by XRD.
Prior to the catalytic tests, all of the samples were activated at 770 K for 4 h in an air flow. The catalytic reaction of N2O decomposition was studied in a flow setup at 620–900 K and an N2O + He (1:1) flow rate of 20–60 mL/min. The sample loading was 0.2 g. The catalyst (0.5–1 mm particle size) was diluted with quartz (1:1). The reaction products and unreacted N2O were analyzed by gas chromatography (a Krystalux chromatograph) using a 1-m Porapak Q column. The only products of N2O decomposition were N2 and O2. Diffuse-reflectance IR spectra were measured in the range of 4000–8000 and 2000–4000 cm−1 with a Beckman Acta-M-VII; and Perkin-Elmer 580 B spectrophotometer, respectively, according to the reported procedures [28]. Molecular hydrogen adsorbed at 77 K and a pressure of 30 Torr were used as a probe for coordinatively unsaturated cations [28,29]. Nitrous oxide was adsorbed on the samples at 300 K and a pressure of 10–30 Torr.
XP spectra were measured with a XSAM-800 spectrometer using the MgKa excitation. The C1S line at 285.0 eV was used as a reference.

4. Conclusions

In conclusion, the obtained catalytic and spectroscopic data allow the arrangement of the systems under study in the following sequence, and according to their performance in N2O decomposition: Zn/HZSM-5 > TS-1 (III) > Cu/HZSM-5 > TS-1 (IV) > (Co, Fe)/Cr/Cu/Al2O3 > HZSM-5 > TS-1 (I), TS-1 (II), TiO2-SiO2. In addition, from these data, two new catalytic compositions, i.e., ZnO/HZSM-5 and Ti-silicalite, with a moderate Si/Ti ratio, exhibit a better performance in the reaction of N2O decomposition, as compared with the conventional Cu-containing zeolite and oxide catalysts. The key role played by coordinatively unsaturated Zn, Cu or Ti ions, as non-framework (Zn, Cu) or framework ions in the N2O decomposition has been revealed. Even the dehydroxylated HZSM-5 zeolite, containing rather strong Lewis acid sites (but still weaker than those in Zn/HZSM-5 catalysts), is more active in the reaction of N2O decomposition compared with the conventionally calcined HZSM-5 zeolite, which contains predominantly Bronsted acid sites. Furthermore, a considerably high N2O conversion reaching 85% is observed for the most active catalysts (Zn/HZSM-5) under rather mild reaction conditions (T = 620 K).

Author Contributions

Conceptualization, L.M.K. and S.F.D.; methodology, A.L.K.; investigation, A.L.K.; writing—original draft preparation, L.M.K.; writing—review and editing, L.M.K. All authors have read and agreed to the published version of the manuscript.

Funding

This work was supported by the Institute of Organic Chemistry of the Russian Academy of Sciences (Program of supporting scientific schools).

Institutional Review Board Statement

Not applicable.

Informed Consent Statement

Not applicable.

Data Availability Statement

Not applicable.

Conflicts of Interest

The authors declare no conflict of interest.

Sample Availability

Samples of the modified ZSM-5 zeolites and titanosilicates are available from the authors.

References

  1. Zholobenko, V.L.; Senchenya, I.N.; Kustov, L.M.; Kazansky, V.B. Complexation and decomposition of N2O on Broensted acid sites in high-silicon zeolites. Spectral and quantum chemical study. Kinet. Catal. 1991, 32, 151–157. [Google Scholar]
  2. Zholobenko, V.L.; Kustov, L.M.; Kazansky, V.B. The role of Lewis acid sites in adsorption and activation of oxygen in redox type reactions on zeolites. In Proceedings of the of the 9th International Zeolite Conference, Boston, MA, USA, 5–10 July 1992; Volume 2, pp. 299–302. [Google Scholar]
  3. Ono, Y.; Tohmori, K.; Suzuki, S.; Nakashiro, K.; Suzuki, E. Functionalization of benzene by its reaction with nitrogen oxides over solid-acid catalysts. Stud. Surf. Sci. Catal. 1998, 41, 75–82. [Google Scholar]
  4. Uriarte, A.K.; Rodkin, M.A.; Gross, M.J.; Kharitonov, A.S.; Panov, G.I. Direct hydroxylation of benzene to phenol by nitrous oxide. Stud. Surf. Sci. Catal. 1997, 110, 857–864. [Google Scholar]
  5. Panov, G.I.; Sobolev, V.L.; Kharitonov, A.S. The role of iron in N2O decomposition on ZSM-5 zeolite and reactivity of the surface oxygen formed. J. Molec. Catal. 1990, 61, 85–97. [Google Scholar] [CrossRef]
  6. Sun, K.; Xia, H.; Feng, Z.; van Santen, R.; Hensen, E.; Li, C. Active sites in Fe/ZSM-5 for nitrous oxide decomposition and benzene hydroxylation with nitrous oxide. J. Catal. 2008, 254, 383–396. [Google Scholar] [CrossRef]
  7. Wilczkowska, E.; Krawczyk, K.; Petryk, J.; Sobczak, J.W.; Kaszkur, Z. Direct nitrous oxide decomposition with a cobalt oxide catalyst. Appl. Catal. A General 2010, 389, 165–172. [Google Scholar] [CrossRef]
  8. Abu-Zied, B.M. Nitrous oxide decomposition over alkali-promoted magnesium cobaltite catalysts. Chinese J. Catal. 2011, 32, 264–272. [Google Scholar] [CrossRef]
  9. Iwanek, E.; Krawczyk, K.; Petryk, J.; Sobczak, J.W.; Kaszkur, Z. Direct nitrous oxide decomposition with CoOx-CeO2 catalysts. Appl. Catal. B Environ. 2011, 106, 416–422. [Google Scholar] [CrossRef]
  10. Kim, M.-J.; Lee, S.-J.; Ryu, I.-S.; Jeon, M.-W.; Jeon, S.G. Catalytic decomposition of N2O over cobalt based spinel oxides: The role of additives. J. Molec. Catal. 2017, 442, 202–207. [Google Scholar] [CrossRef]
  11. Esteves, P.; Wu, Y.; Dujardin, C.; Dongare, M.K.; Granger, P. Ceria-zirconia mixed oxides as thermal resistant catalysts for the decomposition of nitrous oxide at high temperature. Catal. Today 2011, 176, 453–457. [Google Scholar] [CrossRef]
  12. Nunotani, N.; Nagai, R.; Imanaka, N. Direct catalytic decomposition of nitrous oxide gas over rhodium supported on lanthanum silicate. Catal. Commun. 2016, 87, 53–56. [Google Scholar] [CrossRef]
  13. Wang, Y.; Zhang, J.; Zhu, J.; Yin, J.; Wang, H. Experimental research on catalytic decomposition of nitrous oxide on supported catalysts. Energy Convers. Manag. 2009, 50, 1304–1307. [Google Scholar] [CrossRef]
  14. Pachatouridou, E.; Papista, E.; Iliopoulou, E.F.; Delimitis, A.; Goula, G.; Yentekakis, I.V.; Marnellos, G.E.; Konsolakis, M. Nitrous oxide decomposition over Al2O3 supported noble metals (Pt, Pd, Ir): Effect of metal loading and feed composition. J. Environ. Chem. Eng. 2015, 3, 815–821. [Google Scholar] [CrossRef]
  15. Namuangruk, S.; Khongpracha, P.; Tantirungrotechai, Y.; Limtrakul, J. Decomposition of nitrous oxide on carbon nanotubes. J. Molec. Graph. Model. 2007, 26, 179–186. [Google Scholar] [CrossRef] [PubMed]
  16. Lin, F.; Andana, T.; Wu, Y.; Szanyi, J.; Wang, Y.; Gao, F. Catalytic site requirements for N2O decomposition on Cu-, Co-, and Fe-SSZ-13 zeolites. J. Catal. 2021, 401, 70–80. [Google Scholar] [CrossRef]
  17. Wang, S.; Yan, B.; Chai, J.; Li, T.; Yu, H.; Li, T.; Cao, P.; Yang, F.; Yuan, X.; Yin, H. Rhodium Encapsulated within Silicalite-1 Zeolite as Highly Efficient Catalyst for Nitrous Oxide Decomposition: From Single Atoms to Nanoclusters and Nanoparticles. Eur. J. Inorg. Chem. 2021, 23, 2201–2210. [Google Scholar] [CrossRef]
  18. Liu, N.; Zhang, R.; Chen, B.; Li, Y.; Li, Y. Comparative study on the direct decomposition of nitrous oxide over M (Fe, Co, Cu)–BEA zeolites. J. Catal. 2012, 294, 99–112. [Google Scholar] [CrossRef]
  19. Cürdaneli, P.E.; Özkar, S. Ruthenium(III) ion-exchanged zeolite Y as highly active and reusable catalyst in decomposition of nitrous oxide to sole nitrogen and oxygen. Micropor. Mesopor. Mater. 2014, 196, 51–58. [Google Scholar] [CrossRef]
  20. Zhang, X.; Guan, Y.; Zhang, S.; Yang, M.; Zhao, Y.; Hao, Z. Effective catalytic decomposition of nitrous oxide over highly active and stable bimetallic CoIn-mordenite zeolite. J. Molec. Catal. Chem. 2014, 395, 202–209. [Google Scholar] [CrossRef]
  21. Bols, M.L.; Snyder, B.E.R.; Rhoda, H.M.; Cnudde, P.; Fayad, G.; Schoonheydt, R.A.; Van Speybroeck, V.; Solomon, E.I.; Sels, B.F. Coordination and activation of nitrous oxide by iron zeolites. Nat. Catal. 2021, 4, 332–340. [Google Scholar] [CrossRef]
  22. Nakamura, M.; Mitsuhashi, H.; Takezawa, N. Oxygen species formed on different surface sites of CaO by decomposition of N2O and the reactivity. J. Catal. 1992, 138, 686–693. [Google Scholar] [CrossRef]
  23. Tan, S.A.; Grant, R.B.; Lambert, R.M. The silver-catalysed decomposition of N2O and the catalytic oxidation of ethylene by N2O over Ag(111) and Ag/α-Al2O3. J. Catal. 1987, 104, 156–163. [Google Scholar] [CrossRef]
  24. Tabor, E.; Sádovská, G.; Bernauer, M.; Sazama, P.; Nováková, J.; Fíla, V.; Kmječ, T.; Kohout, J.; Závěta, K.; Sobalík, Z. Feasibility of application of iron zeolites for high-temperature decomposition of N2O under real conditions of the technology for nitric acid production. Appl. Catal. Environ. 2019, 240, 358–366. [Google Scholar] [CrossRef]
  25. Kustov, L.M.; Khodakov, A.Y.; Kazansky, V.B. On the Nature of Active Sites for Dehydrogenation of Saturated Hydrocarbons in HZSM-5 Zeolites Modified by Zinc and Gallium Oxides. Stud. Surf. Sci. Catal. 1989, 49B, 1173–1178. [Google Scholar]
  26. Kazansky, V.B.; Kustov, L.M.; Borovkov, V.Y. Near infrared diffuse reflectance study of high silica containing zeolites. Zeolites 1983, 3, 77–81. [Google Scholar] [CrossRef]
  27. Bai, R.; Song, Y.; Bai, R.; Yu, J. Creation of Hierarchical Titanosilicate TS-1 Zeolites. Adv. Mater. Interfaces 2021, 8, 2001095. [Google Scholar] [CrossRef]
  28. Kustov, L.M. New trends in IR-spectroscopic characterization of acid and basic sites in zeolites and oxide catalysts. Topics Catal. 1997, 4, 131–144. [Google Scholar] [CrossRef]
  29. Přech, J. Catalytic performance of advanced titanosilicate selective oxidation catalysts—A review. Catal. Rev. Sci. Eng. 2018, 60, 71–131. [Google Scholar] [CrossRef]
  30. Perego, G.; Bellussi, G.; Carati, A.; Millini, R. Isomorphous Substitution in Zeolite Catalysts. Stud. Surf. Sci. Catal. 1989, 44, 237–238. [Google Scholar]
  31. Tatsumi, T.; Nakamura, M.; Negishi, S.; Tominaga, H. Shape-selective oxidation of alkanes with H2O2 catalysed by titanosilicate. J. Chem. Soc. Chem. Commun. 1990, 6, 476–477. [Google Scholar] [CrossRef]
  32. Vaccaro, L.; Cannas, M.; Radzig, V. Luminescence properties of nonbridging oxygen hole centers at the silica surface. J. Non-Crystal. Solids 2009, 355, 1020–1023. [Google Scholar] [CrossRef]
Figure 1. IR spectra of H2 adsorbed at 77 K on: (1) Dehydroxylated HZSM-5 zeolite; (2) Cu/HZSM-5; (3) Zn/HZSM-5.
Figure 1. IR spectra of H2 adsorbed at 77 K on: (1) Dehydroxylated HZSM-5 zeolite; (2) Cu/HZSM-5; (3) Zn/HZSM-5.
Molecules 27 00398 g001
Figure 2. (1) IR spectra of N2O adsorbed at 300 K on Zn/HZSM-5; (2) IR spectra upon heating the Zn/HZSM-5 zeolite at 520 K for 1 h with pre-adsorbed N2O (300 K).
Figure 2. (1) IR spectra of N2O adsorbed at 300 K on Zn/HZSM-5; (2) IR spectra upon heating the Zn/HZSM-5 zeolite at 520 K for 1 h with pre-adsorbed N2O (300 K).
Molecules 27 00398 g002
Scheme 1. Mechanism of N2O decomposition on Lewis acid-base pair sites.
Scheme 1. Mechanism of N2O decomposition on Lewis acid-base pair sites.
Molecules 27 00398 sch001
Figure 3. Representative XP spectra: (1) TS-1(I) (Si/Ti = 14.4); (2) TS-1 (II) (Si/Ti = 22.9); (3) TS-1(III) (Si/Ti = 32).
Figure 3. Representative XP spectra: (1) TS-1(I) (Si/Ti = 14.4); (2) TS-1 (II) (Si/Ti = 22.9); (3) TS-1(III) (Si/Ti = 32).
Molecules 27 00398 g003
Scheme 2. Mechanism of N2O decomposition on Ti-centers.
Scheme 2. Mechanism of N2O decomposition on Ti-centers.
Molecules 27 00398 sch002
Figure 4. IR spectra of N2O adsorbed on TS-1 (Si/Ti = 14.4) (a) and TS-1 (Si/Ti = 32) (b) at 300 K (1) and upon heating the samples at 570 K for 1 h with pre-adsorbed N2O (300 K) (2).
Figure 4. IR spectra of N2O adsorbed on TS-1 (Si/Ti = 14.4) (a) and TS-1 (Si/Ti = 32) (b) at 300 K (1) and upon heating the samples at 570 K for 1 h with pre-adsorbed N2O (300 K) (2).
Molecules 27 00398 g004
Table 1. N2O decomposition (45 cm3 N2O/min).
Table 1. N2O decomposition (45 cm3 N2O/min).
CatalystReaction Temperature, KN2O Conversion, %TOF,
mmol N2O g−1 s−1
Conventionally calcined HZSM-5 (770 K)720120.020
Dehydroxylated HZSM-5 (970 K)720550.046
3% Zn/HZSM-5620850.071
645900.075
6601000.084
5% Zn/HZSM-5620850.071
6451000.084
3% Cu/HZSM-5620200.017
645550.046
660850.071
6701000.084
Co/Cr/Cu/Al2O3645450.038
670800.067
Table 2. Results of catalytic testing of various Ti-systems in the reaction of N2O decomposition.
Table 2. Results of catalytic testing of various Ti-systems in the reaction of N2O decomposition.
CatalystSi/TiT, KN2O Flow Rate, cm3/minConversion of N2O, %TOF,
mmol N2O g−1 s−1
TS-1 (I)14.477020150.006
870 200.008
TS-1 (II)22.977020100.004
870 500.019
TS-1 (III)32.062045550.046
645 800.067
670 850.071
TS-1 (IV)37.962045450.038
645 600.050
670 800.067
TiO2-SiO217.072045100.008
820 500.042
Publisher’s Note: MDPI stays neutral with regard to jurisdictional claims in published maps and institutional affiliations.

Share and Cite

MDPI and ACS Style

Kustov, L.M.; Dunaev, S.F.; Kustov, A.L. Nitrous Oxide Adsorption and Decomposition on Zeolites and Zeolite-like Materials. Molecules 2022, 27, 398. https://0-doi-org.brum.beds.ac.uk/10.3390/molecules27020398

AMA Style

Kustov LM, Dunaev SF, Kustov AL. Nitrous Oxide Adsorption and Decomposition on Zeolites and Zeolite-like Materials. Molecules. 2022; 27(2):398. https://0-doi-org.brum.beds.ac.uk/10.3390/molecules27020398

Chicago/Turabian Style

Kustov, Leonid M., Sergey F. Dunaev, and Alexander L. Kustov. 2022. "Nitrous Oxide Adsorption and Decomposition on Zeolites and Zeolite-like Materials" Molecules 27, no. 2: 398. https://0-doi-org.brum.beds.ac.uk/10.3390/molecules27020398

Article Metrics

Back to TopTop