Next Article in Journal
Efficient and Selective Removal of Palladium from Simulated High-Level Liquid Waste Using a Silica-Based Adsorbent NTAamide(C8)/SiO2-P
Previous Article in Journal
A Novel PDMS-Based Flexible Thermoelectric Generator Fabricated by Ag2Se and PEDOT:PSS/Multi-Walled Carbon Nanotubes with High Output Performance Optimized by Embedded Eutectic Gallium–Indium Electrodes
Previous Article in Special Issue
Analytical Modeling and Optimization of Cu2ZnSn(S,Se)4 Solar Cells with the Use of Quantum Wells under the Radiative Limit
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

Fabrication of Pre-Structured Substrates and Growth of CIGS Micro-Absorbers

1
International Iberian Nanotechnology Laboratory, Av. Mestre José Veiga s/n, 4715-330 Braga, Portugal
2
Centre of Physics of Minho and Porto Universities (CF-UM-UP), Azurém Campus, University of Minho, 4800-058 Guimarães, Portugal
*
Authors to whom correspondence should be addressed.
Submission received: 20 February 2024 / Revised: 14 March 2024 / Accepted: 18 March 2024 / Published: 20 March 2024
(This article belongs to the Special Issue State-of-the-Art Nanomaterials for Solar Cells)

Abstract

:
Second-generation thin-film Cu(In, Ga)Se2 (CIGS) solar cells are a well-established photovoltaic technology with a record power conversion efficiency of 23.6%. However, their reliance on critical raw materials, such as In and Ga, requires new approaches to reduce the amount of critical raw materials employed. The micro-concentrator concept involves the combination of thin-film photovoltaic technology with concentrator photovoltaic technology. This approach reduces the size of the solar cell to the micrometer range and uses optical concentration to collect sunlight from a larger area, focusing it onto micro solar cells. This work is devoted to the development of a process for manufacturing pre-structured substrates with regular arrays of holes with 200 and 250 µm diameters inside a SiOx insulating matrix. Subsequently, a Cu–In–Ga precursor is deposited by sputtering, followed by photoresist lift-off and the application of a Cu–In–Ga thermal annealing at 500 °C to improve precursor quality and assess pre-structured substrate stability under elevated temperatures. Finally, a two-stage selenization process leads to the formation of CIGS absorber micro-dots. This study presents in detail the fabrication process and explores the feasibility of a bottom-up approach using pre-structured substrates, addressing challenges encountered during fabrication and providing insights for future improvements in CIGS absorber materials.

1. Introduction

From 2021 to 2022, global photovoltaic installations increased from 175 GW to 240 GW, an overall growth of 65 GW. China dominated the market, installing 106 GW in 2022, corresponding to 44% of the global market. The European Union followed, installing 38.7 GW, led by Spain (8.1 GW), Germany (7.5 GW), Poland (4.9 GW), and the Netherlands (3.9 GW) [1]. For 2023, analysts project a substantial increase, estimating that photovoltaic installations could reach approximately 440 GW, double that of 2022 [2]. In 2021, crystalline-silicon (c-Si) photovoltaics represented a 95% share of production [3]. This technology achieved record efficiencies of 26.8% for mono-crystalline, 24.4% for multi-crystalline, and 27.6% for concentrator mono-crystalline [4,5]. To further enhance efficiency, new PV cell architectures like PERC (Passivated Emitter and Rear Cell) [6] have been explored. The main difference from a typical monocrystalline silicon cell lies in the inclusion of a passivation layer (a dielectric material) on the back cell’s surface, promoting an increase in the efficiency of the PV solar cell. Thin-film solar cells have emerged as a compelling and cost-efficient alternative to c-Si. Recently, Keller et al. [7] reported a 23.6% record efficiency for non-concentrated (Ag,Cu)(In,Ga)Se2 solar cells by introducing Ag into the absorber, implementing a Ga profile with a high concentration of Ga close to the back contact and lower concentration closer to the CdS buffer layer, and a post-deposition treatment with RbF. Ward et al. [8] presented CIGS concentrator cells grown by physical evaporation using a modified three-stage process, achieving an efficiency of 20.8% under 1 sun and a record efficiency of 23.3% at 14.7 suns. Furthermore, CdTe solar cells have achieved an efficiency of 22.3% [5].
Concentrator photovoltaic (CPV) technology uses optical elements such as mirrors and/or lenses to concentrate light onto small and highly efficient solar cells [9], aiming to enhance overall performance. An ideal CPV system incorporates cost-efficient concentrating optics to reduce the active solar cell area, enabling the use of more expensive, high-efficiency solar cells [10]. Remarkable efficiencies of 47.6% at 665 suns [11] and 30.8% at 61 suns [12] have been achieved for four-junction (GaInP/GaInAs; GaInAsP/GaInAs) and flexible GaAs solar cells, respectively.
To enhance power conversion efficiency (PCE), reduce material usage, and lower costs, micro-concentrator photovoltaics (micro-CPVs) have been intensively investigated in recent years [10,13,14]. The micro-CPV concept consists of reducing the solar cells’ lateral dimensions to the range of hundreds of micrometers, resulting in cell areas below 1 mm2 [14,15]. Thin-film micro-CPVs present several advantages over conventional CPVs and other technologies, including enhanced cell performance, material savings, efficient thermal management, reduced series resistance losses, and thinner modules [16]. Through simulations, Sadewasser et al. [17] demonstrated that micro-concentrator solar cells offer a substantial advantage over regular CPV devices. The smaller size of devices leads to improved heat management, and for micro solar cells with a diameter of <200 µm, the temperature can be kept at less than 10 °C above the temperature of a flat panel solar cell. Paire et al. [18] showed that reducing cell size to the micrometric range allows better thermal evacuation due to a higher surface-to-volume ratio and reduced resistance losses. The microcells showed a 4% absolute improvement in efficiency at a concentration ratio of ×120, increasing from 13% to 17%. Under a concentration of ×1000, the microcells with a diameter under 50 µm had a temperature increase of less than 20 K.
In recent years, CIGS micro-CPVs have attracted increasing attention, and significant progress has been made, demonstrating the feasibility of the CIGS micro-concentrator concept. The required micro-CIGS solar cells can be fabricated using either a top-down or bottom-up approach.
The top-down approach involves isolating the microcells within a large-area solar cell by shadowing, selective deposition, or isolation. Paire et al. [19] fabricated a device with a glass–Mo–CIGS–CdS–ZnO structure featuring a 15-micrometer-diameter active area, with an efficiency of 17% at ×120. The microcells were created by depositing a 400-nanometer-thick insulating SiO2 layer and a 20 nm/300 nm Ti/Au bilayer on top of the buffer layer. The holes in the SiO2 layer were defined by photolithography, after which the ZnO window layer was deposited. In 2013, Paire [20] prepared the CIGS absorber by co-evaporation, creating microcells with a 50-micrometer diameter using photolithography and achieving an efficiency of 21.3% at ×475. In a subsequent study [21], CIGS mesa microcells were fabricated through chemical etching. First, an array of patterned photoresist was coated on the cell surface. Then, the front window and CdS layers were etched with a hydrochloric acid solution. Finally, the CIGS layer was chemically etched with a bromine-based solution. The resulting devices exhibited an average absolute efficiency increase of 2% per concentration decade up to approximately 1000 suns. Reinhold et al. [22] developed lamellar-shaped micro solar cells with monolithic interconnects through standard P1, P2, and P3 scribes. This patterning allows a serial connection of single solar cells to form a solar module. The Mo back contact was divided with a P1-scribe, followed by a P2-scribe into the CIGS layer. Finally, a P3-scribe separates the front contact between two cells. The P1-scribe was made using a laser, while the P2 and P3 were mechanically scribed. The lamellar microcells can have an absolute 3.8% efficiency increase under concentrated white light.
In the bottom-up approach, the absorber is locally grown in patterned/defined areas by using masks, patterned substrates, or pre-structured substrates, thereby reducing the usage of critical materials. While various methods can be used to deposit large-area CIGS absorbers, not all allow for local absorber growth. According to the literature, material-efficient deposition methods for CIGS or CuInSe2 (CIS) micro-absorbers include electrodeposition, physical vapor deposition (PVD), and laser-induced forward transfer. Ringleb et al. [23] demonstrated the growth of CIS and CIGS by nucleation of In droplets on laser-patterned substrates during physical vapor deposition and by laser-induced forward transfer (LIFT) of Cu, In, and Ga precursor layers. Efficiencies of 3.06% at 3 suns and 3.36% at 20 suns were achieved for the CIS and CIGS microcells from the nucleation approach, while the CIGS microcells from the LIFT approach reached 0.237% at 20 suns. Heidmann et al. [24] were able to grow CIS micro-absorbers without using patterned substrates by local growth of In islands on Mo-coated glass by PVD, followed by deposition of copper and subsequent selenization, reaching an efficiency of 2.9% under 1 sun and 3.1% at 3 suns. Correia et al. [25] deposited CIS on patterned substrates by electrodeposition, achieving an efficiency of 4.8% under 1 sun. Siopa et al. [26] electrodeposited CIGS absorber layers of 500- and 1500-nanometers-thick into micro-patterned substrates. The microcells demonstrated an increase in efficiencies, reaching 4.8% at 33 suns for the 500-nanometer-thick layer and 5.2% at 3 suns for the 1500-nanometer-thick layer. Table 1 provides a summary of both top-down and bottom-up fabrication approaches for CIGS micro solar cells.
Despite the numerous potential benefits, micro-CPVs also present challenges that need to be addressed. Domínguez et al. [14] have described difficulties related to the components’ size, emphasizing the crucial need for accuracy and precision in manufacturing, manipulation, alignment, and connection of the microcells and micro-optics. Furthermore, the size of these elements can limit the use of specific tools. Achieving large-scale production at low cost requires the development of enabling manufacturing processes already used in the industries for parallel assembly and interconnection of solar cells, such as self-assembly or inkjet printing, along with large-area optical fabrication methods like hot embossing or casting. Additionally, exploring unconventional optical architectures or reconsidering conventional concepts previously discarded due to high material consumption or high bulk absorption at standard CPV might be viable alternatives. An investigation of CIGS micro-CPVs will enable further understanding of the cell materials’ quality, physical and photovoltaic parameters, as well as their operation principles and limitations. This work aims to present a bottom-up approach for the fabrication of pre-structured substrates developed through photolithography and the growth of CIGS micro-absorbers. This study details the process step-by-step, highlighting key parameters and outlining considerations in substrate fabrication.

2. Materials and Methods

Fabrication started with cleaning 1-millimeter-thick soda–lime glass (SLG) substrates using ultrasonic baths with detergent and deionized water. In the first bath, deionized water at room temperature was used with 3 mL of detergent (MicroSon, FisherbrandTM, Fisher Scientific, Landsmeer, The Netherlands) for 10 min. The second bath was performed at 60 °C with detergent for 10 min. From the third to sixth bath, no detergent was used.
Next, a 500-nanometer-thick Mo back contact bilayer was deposited onto the cleaned SLG substrates by DC magnetron sputtering in the STAR (Sputtering for Advanced Research) sputter-deposition system [27]. To achieve good adhesion of the Mo film to the SLG substrate, a 100-nanometer layer was deposited at 1 Pa pressure, followed by a 400-nanometer layer deposited under a pressure of 0.7 Pa to ensure good conductivity.

2.1. Pre-Structured Substrate Fabrication

The pre-structured substrates (Figure 1) were fabricated in a cleanroom environment, primarily designed for Si wafers, requiring adaptations for using 5 × 5 cm2 SLG substrates. The process began with another cleaning step in an ultrasonic bath with acetone, followed by several isopropyl alcohol (IPA) and deionized water rinses. Then, the substrate was vapor-primed in an oven (310TA, Yield Engineering Systems, Inc., Fremont, CA, USA) to remove water and organic residues.
Next, a 2-micrometer-thick SiOx layer was deposited using plasma-enhanced chemical vapor deposition (MPX CVD Module, SPTS Technologies Ltd., Newport, UK) at 300 °C, with a ~45 nm/min deposition rate. Afterward, the substrate SLG–Mo–SiOx is vapor primed with hexamethyldisilazane (HMDS) in the oven prior to the photoresist coating to enhance adhesion to the substrate. Then, a 2200-nanometer-thick positive photoresist layer (AZ4110, Merck KGaA, Darmstadt, Germany) was spin-coated onto the SiOx layer. The micro-dot pattern was exposed by a direct write laser (DWL 2000, Heidelberg Instruments GmbH, Heidelberg, Germany) lithography system, using a laser power of 120 mW and 405 nm wavelength, followed by the photoresist development (AZ400K 1:4, Merck KGaA, Darmstadt, Germany). Alternatively, a mask aligner (MA6BA6, Suss MicroTec, Garching, Germany) was also used for pattern exposure. The DWL creates high-resolution patterns by laser writing directly onto photoresist-coated samples, whereas the mask aligner requires a physical mask to transfer the pattern. In this case, the mask aligner exposure was performed using a 405 nm wavelength and a low-resolution acetate mask instead of a high-resolution acetate or hard mask. The mask aligner had an exposure time of seconds, whereas, for the DWL, it was at least 10 min. The pattern matrix consisted of circular areas of 200- and 250-micrometer diameters with a 2000-micrometer pitch (Figure 2). Furthermore, a test area of 0.012 mm2 was incorporated for characterization purposes.
Subsequently, the micro-holes were etched through the SiOx layer by reactive ion etching (RIE) (APS Module, SPTS, Technologies Ltd., Newport, UK) until reaching the Mo back contact layer, which was confirmed through optical microscope inspections and profilometer measurements. Once the etching is completed, two routes can be considered to finish the substrate and deposit the Cu–In–Ga (CIG) precursor. In the first, employed in this work, a CIG layer was grown by sputtering followed by photoresist lift-off, leaving the SiOx layer with the CIG inside the micro-holes. Subsequently, a plasma asher (M360, PVA TePla America Inc., Corona, CA, USA) was used to remove any residual photoresist. The lifted-off material can be subjected to recovery and recycling processes to produce new targets or to separate the CIG materials [28]. The second route involves area-selective deposition or local growth methods, such as electrodeposition [25,26,29], which are recommended for material saving. In this approach, the photoresist removal is performed after the deposition process.

2.2. Structuring the Substrate

To accommodate the use of 5 × 5 cm2 SLG substrates in the cleanroom, where most tools are prepared to handle 8-inch diameter Si wafers, specific sample-mounting adaptations were necessary for the SiOx deposition, photoresist coating and development (Figure 3a), and SiOx etching (Figure 3b,c).
For photoresist coating, the SLG–Mo–SiOx substrate is fixed on a Si wafer with Kapton tape (Figure 3a). Afterward, for SiOx RIE, a crystalbond wax was used between the Si wafer and the SLG pre-structured substrate for good thermal uniformity. Kapton tape was placed around the substrate to fix it against the Si wafer and maintain the wax (which melts during the SiOx etching process) between the SLG and the Si support wafer (Figure 3b). Also, the pre-structured substrate was mounted on a Si wafer next to an un-processed SLG substrate for proper weight distribution and effective wafer handling in the RIE tool.

2.3. CIG Precursor Deposition followed by 2-Stage Selenization

The CIG precursor was deposited from a ternary CIG target (50:35:15 at%, Testbourne) by the magnetron sputtering system STAR [27] at 1.5 W/cm2 power density under Ar atmosphere at a working pressure of 0.55 Pa. Subsequently, the resist was removed by lift-off with acetone followed by plasma asher treatment to eliminate any residual photoresist, leaving the SiOx layer with the CIG micro-dots. To prevent Mo oxidation, which starts at 300 °C, a low-temperature plasma asher process was employed.
Thermal annealing was introduced prior to selenization to remove any possible photoresist incorporated into the CIG micro-dot during sputtering [30], to improve the precursor quality. Hence, the sample was placed inside a vacuum pot and placed on a heating plate. To prevent contamination, nitrogen was purged and pumped three times into the pot. Then, the hotplate temperature was set to 500 °C and kept for 30 min once the desired temperature was reached. It is important to note that the temperature inside the vacuum pot was lower than the nominal temperature at the hot plate.
The CIG precursor was selenized inside a closed graphite box with 50 mg of Se pellets, and loaded inside a quartz tube to obtain the CIGS absorber. The tube underwent a few cycles of nitrogen and argon purging and pumping to minimize the risk of oxygen contamination. During the 2-stage selenization process, in the first stage, the temperature was kept at 100 °C for 30 min to homogenize the precursors. Subsequently, the temperature was increased to 480 °C for 30 min. Once the process was complete, the furnace was cooled down to below 130 °C. A continuous flow of 100 sccm of Ar was maintained throughout the entire process. Furthermore, both heating and cooling ramps were fixed at a slope of 10 and 20 °C/min, respectively. The heating profile of the selenization process is shown in Figure 4. Furthermore, after selenization, a KCN etching (5%) was performed, followed by CdS buffer layer deposition using a chemical bath.

2.4. Characterization Methods

The electrical properties of the Mo bilayer were evaluated through 4-point probe measurements before and after the fabrication process to ensure the integrity and functionality of the film. To confirm the dimensions and depth of the micro-holes, optical microscope images and profilometer measurements were conducted during the fabrication process.
The morphologies and elemental composition analysis of the as-deposited CIG precursor, annealed ones, and CIGS micro-dots were obtained by scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDX) in a FEI Quanta 650 FEG (FEI Company, Hillsboro, OR, USA) SEM coupled with an EDX detector. Raman spectroscopy was performed using a confocal Raman microscope (WITec Alpha 300 R, WITec Wissenschaftliche Instrumente und Technologie GmbH, Ulm, Germany) using a 532 nm laser excitation.

3. Results and Discussion

3.1. Pre-Structured Substrate

To ensure a well-conducting back contact for the CIGS solar cell, the sheet resistance of the Mo bilayer was measured both before and after the fabrication. This measurement also confirms that the SiOx layer was properly etched, reaching the Mo layer. A consistent sheet resistance of (1.5 ± 0.3) Ohm/sq was measured before and after the fabrication, confirming the integrity of the electrical properties of the Mo film.
The choice of tools for the photoresist exposure of the pattern significantly influences the definition and resolution of the micro-holes in the fabrication process. The photoresist exposure using DWL yielded a higher resolution compared to that achieved with a mask aligner, as illustrated in Figure 5a,b. In the latter case, the final pattern’s low resolution can be explained by the intrinsic low resolution of the acetate-printed photomask coupled with the non-optimal contact between the acetate and the glass slide supporting it for mask aligner use. The SEM micrographs show the successful transfer of the mask pattern to the photoresist using DWL (Figure 5e) and the mask aligner (Figure 5f), along with the resulting micro-holes after SiOx etching.
During the RIE process, optical microscopy inspection and profilometer measurements were conducted after each run to verify if the SiOx was completely etched. In Figure 5c, the micro-holes exhibit different colors, indicating slight variations in the SiOx layer thickness after a SiOx etching run. Figure 5d shows a fully etched micro-hole. In some cases, additional SiOx etching runs were necessary to achieve the desired results. While the etching rate of SiOx on standard Si wafers is typically 274 nm/min, on this substrate, the etching rate decreased and became non-uniform, requiring further characterization after each run. This discrepancy could be ascribed to the uneven wax spread during the sample mounting and to trapped air bubbles (Figure 3c), which may lead to thermal non-uniformity and variations in the etching rate. It is crucial to note that the etching process was performed multiple times, with each run lasting a maximum of 4 min, as etching for a longer time can result in the photoresist burning.

3.2. CIGS Growth

Figure 6 shows the surface and cross-sectional micrographs of sputtered CIG precursor micro-dots prior to the photoresist removal. The CIG precursor exhibits a rough surface, with Cu–In-rich grains/islands distributed on the film’s surface. The elemental ratios CGI = [Cu]/([In] + [Ga]) and GGI = [Ga]/([Ga] + [In]) were determined through EDX measurements. The target composition corresponds to the CGI and GGI ratios of 1 and 0.3, respectively. However, due to the sputtering target usage and potential cross-contamination from other targets, these ratios can vary in the deposited films. Consequently, the aimed CIG precursor ratios are defined as 0.7 < CGI < 1 and 0.2 < GGI < 0.3. The precursor film is found to be Cu-poor, with a CGI of 0.88 ± 0.04 and GGI of 0.26 ± 0.02, both within the desired ranges. SEM micrographs and EDX measurements were performed at the same micro-dots after thermal annealing and selenization to obtain reliable data.
Figure 7 shows SEM micrographs of the as-deposited CIG film (Figure 7a) and annealed at 500 °C (Figure 7b). In the annealed CIG film, the Cu–In-rich grains appear less distinct compared to the as-deposited CIG, and small areas reveal Mo exposure, which could be related to the degassing of photoresist incorporated during CIG sputtering or debris that was not completely removed after RIE. Notably, the SiOx layer remained intact after the annealing process. The average CGI and GGI ratios for the analyzed micro-dots are 0.84 ± 0.05 and 0.28 ± 0.03, respectively, falling within the expected ranges.
The thermally annealed CIG film underwent a two-stage selenization process at 100 and 480 °C. The SEM micrographs showcase the as-deposited CIG precursor (Figure 8a–d), annealed at 500 °C (Figure 8b–e), and the resulting CIGS micro-dots (Figure 8c–f). The surface of the CIGS micro-dot appears rough and homogenous throughout the micro-dot. It is important to highlight that Figure 8f was acquired following the CdS deposition. A summarized elemental composition is presented in Table 2. The CGI ratio was slightly higher than desired, which can be detrimental to the absorber quality. In high-efficiency solar cells, the CIGS absorber requires a low Ga atomic ratio, approximately 0.2–0.3, and a CGI ratio within the range of 0.88–0.92 [31].
In Figure 9, the Raman spectra of a CIGS micro-absorber reveal dominant peaks centered at about 175 and 300 cm−1. The peak at 175 cm−1 corresponds to the A1 Raman peak of CIGS, associated with the presence of the I-II-VI2 chalcopyrite compounds [32]. This peak has a full width at half maximum (FWHM) of 6.5 cm−1, indicating a high crystalline quality of the CIGS layer, which is slightly higher but comparable to the FWHM of 3.7 cm−1 obtained from a reference single crystal Si sample. Furthermore, the shoulder near 260 cm−1 could be attributed to the presence of Cu-Se compounds such as CuSe or Cu2Se [32,33]. The peak at 300 cm−1 has been identified as the main Raman peak from the CdS buffer layer. After the selenization process, the SiOx layer exhibited some cracking (see red rectangles in Figure 8c), whereas the CIGS micro-dots appeared to remain intact. Given the absence of damage after thermal annealing and in comparable samples after selenization, we hypothesize that mechanical stress incurred during the sample’s breaking into smaller pieces led to cracks during selenization.

4. Conclusions

In this study, we present a detailed fabrication process and successfully demonstrate the feasibility of employing a bottom-up approach using pre-structured substrates developed through photolithography for micro-concentrator applications. This approach allows easy modifications to the pattern design for different structures and geometries.
The choice of method for photoresist exposure significantly influences the resolution and definition of the micro-holes, with a direct-write laser resulting in higher resolution compared to a mask aligner. The use of a high-resolution acetate or hard mask should improve the exposure resolution but in both cases no modifications to the pattern designs are possible.
While the fabrication process required some adaptations, the major challenge was encountered during the SiOx etching process, which required intensive inspection after each run and sometimes multiple etching runs to achieve the desired depth to reach the Mo layer.
CIGS micro-absorbers were prepared via sputtering of the CIG precursor into a patterned SiOx matrix, followed by lift-off, thermal annealing at 500 °C, and a two-stage selenization process. The results indicate that both the as-deposited and annealed CIG films were Cu-poor, with CGI ratios of 0.88 and 0.84, respectively. The surface of the as-deposited CIG film exhibited roughness, characterized by CIG grains throughout the film. Subsequent thermal annealing at 500 °C led to less pronounced grains. After the two-stage selenization, the CIGS film had a CGI ratio of 1 and exhibited Raman spectra with a dominant A1 mode peak at 175 cm−1, observed in I-III-VI2 chalcopyrite compounds. In future work, we aim to improve the CIGS absorber material by optimizing the two-stage selenization temperature and to produce complete CIGS microcells by deposing buffer and window layers.

Author Contributions

Conceptualization, M.A., S.S. and J.C.; formal analysis, M.A.; investigation, M.A. and P.A.; writing—original draft preparation, M.A.; writing—review and editing, M.A., P.A., S.S., J.C. and V.T.; supervision, S.S. and J.C. All authors have read and agreed to the published version of the manuscript.

Funding

This research was funded by Fundação para a Ciência e a Tecnologia (FCT), PhD Scholarship number 2020.06063BD and partially funded by the UIDB/04650/2020 Strategic Project of the Physics Center of the University of Minho and Porto.

Data Availability Statement

The data presented in this study are available on request from the corresponding author.

Acknowledgments

We would like to acknowledge Ricardo Poeira and Phillip Dale at the Department of Physics and Materials Science at the University of Luxembourg for their support.

Conflicts of Interest

The authors declare no conflicts of interest.

References

  1. Masson, G.; Bosch, E.; van Rechem, A.; de I’Epine, M.; Kaizuka, I.; Jäger-Waldau, A.; Donoso, J. Snapshot of Global PV Markets 2023; International Energy Agency, Photovoltaic Power Systems Programme: Paris, France, 2023. [Google Scholar]
  2. Feldman, D.; Zuboy, J.; Dummit, K.; Stright, D.; Heine, M.; Mirletz, H.; Margolis, R. Winter 2024 Solar Industry Update; National Renewable Energy Laboratory (NREL): Golden, CO, USA, 2024. [Google Scholar]
  3. Philipps, S.; Warmuth, W.; Bett, A.W.; Burger, B.; Friedrich, L.; Kost, C.; Nold, S.; Peper, D.; Preu, R.; Rentsch, J.; et al. Photovoltaics Report. Available online: https://www.ise.fraunhofer.de/content/dam/ise/de/documents/publications/studies/Photovoltaics-Report.pdf (accessed on 3 January 2024).
  4. Slade, A.; Garboushian, V. 27.6% Efficient Silicon Concentrator Solar Cells for MassProduction. In Proceedings of the 15th International Photovoltaic Science and Engineering Conference, Shanghai, China, 10–15 October 2005; p. 701. [Google Scholar]
  5. Green, M.A.; Dunlop, E.D.; Yoshita, M.; Kopidakis, N.; Bothe, K.; Siefer, G.; Hao, X. Solar Cell Efficiency Tables (Version 62). Prog. Photovoltaics Res. Appl. 2023, 31, 651–663. [Google Scholar] [CrossRef]
  6. Kashyap, S.; Madan, J.; Pandey, R.; Sharma, R. Comprehensive Study on the Recent Development of PERC Solar Cell. Conf. Rec. IEEE Photovolt. Spec. Conf. 2020, 2020, 2542–2546. [Google Scholar] [CrossRef]
  7. Keller, J.; Kiselman, K.; Donzel-Gargand, O.; Martin, N.M.; Babucci, M.; Lundberg, O.; Wallin, E.; Stolt, L.; Edoff, M. High-Concentration Silver Alloying and Steep Back-Contact Gallium Grading Enabling Copper Indium Gallium Selenide Solar Cell with 23.6% Efficiency. Nat. Energy 2024. [Google Scholar] [CrossRef]
  8. Ward, J.S.; Egaas, B.; Noufi, R.; Contreras, M.; Ramanathan, K.; Osterwald, C.; Emery, K. Cu(In,Ga)Se2 Solar Cells Measured under Low Flux Optical Concentration. In Proceedings of the 2014 IEEE 40th Photovoltaic Specialist Conference (PVSC), Denver, CO, USA, 8–13 June 2014; pp. 2934–2937. [Google Scholar]
  9. Khamooshi, M.; Salati, H.; Egelioglu, F.; Hooshyar Faghiri, A.; Tarabishi, J.; Babadi, S. A Review of Solar Photovoltaic Concentrators. Int. J. Photoenergy 2014, 2014, 958521. [Google Scholar] [CrossRef]
  10. Wiesenfarth, M.; Anton, I.; Bett, A.W. Challenges in the Design of Concentrator Photovoltaic (CPV) Modules to Achieve Highest Efficiencies. Appl. Phys. Rev. 2018, 5, 041601. [Google Scholar] [CrossRef]
  11. Dimroth, F.; Tibbits, T.N.D.; Niemeyer, M.; Predan, F.; Beutel, P.; Karcher, C.; Oliva, E.; Siefer, G.; Lackner, D.; Fus-Kailuweit, P.; et al. Four-Junction Wafer-Bonded Concentrator Solar Cells. IEEE J. Photovoltaics 2016, 6, 343–349. [Google Scholar] [CrossRef]
  12. Kayes, B.M.; Zhang, L.; Twist, R.; Ding, I.K.; Higashi, G.S. Flexible Thin-Film Tandem Solar Cells with >30% Efficiency. IEEE J. Photovoltaics 2014, 4, 729–733. [Google Scholar] [CrossRef]
  13. Paire, M.; Lombez, L.; Guillemoles, J.F.; Lincot, D. Toward Microscale Cu(In,Ga)Se2 Solar Cells for Efficient Conversion and Optimized Material Usage: Theoretical Evaluation. J. Appl. Phys. 2010, 108, 034907. [Google Scholar] [CrossRef]
  14. Domínguez, C.; Jost, N.; Askins, S.; Victoria, M.; Antón, I. A Review of the Promises and Challenges of Micro-Concentrator Photovoltaics. AIP Conf. Proc. 2017, 1881, 080003. [Google Scholar] [CrossRef]
  15. Paire, M.; Lombez, L.; Donsanti, F.; Jubault, M.; Lincot, D.; Guillemoles, J.-F.; Collin, S.; Pelouard, J.-L. Thin-Film Microcells: A New Generation of Photovoltaic Devices. SPIE Newsroom 2013, 5, 2–3. [Google Scholar] [CrossRef]
  16. Alves, M.; Pérez-Rodríguez, A.; Dale, P.J.; Domínguez, C.; Sadewasser, S. Thin-Film Micro-Concentrator Solar Cells. J. Phys. Energy 2020, 2, 012001. [Google Scholar] [CrossRef]
  17. Sadewasser, S.; Salomé, P.M.P.; Rodriguez-Alvarez, H. Materials Efficient Deposition and Heat Management of CuInSe2 Micro-Concentrator Solar Cells. Sol. Energy Mater. Sol. Cells 2017, 159, 496–502. [Google Scholar] [CrossRef]
  18. Paire, M.; Shams, A.; Lombez, L.; Péré-Laperne, N.; Collin, S.; Pelouard, J.L.; Guillemoles, J.F.; Lincot, D. Resistive and Thermal Scale Effects for Cu(In,Ga)Se2 Polycrystalline Thin Film Microcells under Concentration. Energy Environ. Sci. 2011, 4, 4972–4977. [Google Scholar] [CrossRef]
  19. Paire, M.; Lombez, L.; Péré-Laperne, N.; Collin, S.; Pelouard, J.-L.; Lincot, D.; Guillemoles, J.-F. Microscale Solar Cells for High Concentration on Polycrystalline Cu(In,Ga)Se2 Thin Films. Appl. Phys. Lett. 2011, 98, 264102. [Google Scholar] [CrossRef]
  20. Paire, M.; Lombez, L.; Donsanti, F.; Jubault, M.; Collin, S.; Pelouard, J.L.; Guillemoles, J.F.; Lincot, D. Cu(In, Ga)Se2 Microcells: High Efficiency and Low Material Consumption. J. Renew. Sustain. Energy 2013, 5, 011202. [Google Scholar] [CrossRef]
  21. Paire, M.; Jean, C.; Lombez, L.; Collin, S.; Pelouard, J.-L.; Gérard, I.; Guillemoles, J.-F.; Lincot, D. Cu(In,Ga)Se2 Mesa Diodes for the Study of Edge Recombination. Thin Solid Films 2015, 582, 258–262. [Google Scholar] [CrossRef]
  22. Reinhold, B.; Schmid, M.; Greiner, D.; Schüle, M.; Kieven, D.; Ennaoui, A.; Lux-steiner, M.C. Monolithically Interconnected Lamellar Cu(In,Ga)Se2 Micro Solar Cells under Full White Light Concentration. Prog. Photovoltaics Res. Appl. 2015, 23, 1929–1939. [Google Scholar] [CrossRef]
  23. Ringleb, F.; Andree, S.; Heidmann, B.; Bonse, J.; Eylers, K.; Ernst, O.; Boeck, T.; Schmid, M.; Krüger, J. Femtosecond Laser-Assisted Fabrication of Chalcopyrite Micro-Concentrator Photovoltaics. Beilstein J. Nanotechnol. 2018, 9, 3025–3038. [Google Scholar] [CrossRef]
  24. Heidmann, B.; Ringleb, F.; Eylers, K.; Levcenco, S.; Bonse, J.; Andree, S.; Krüger, J.; Unold, T.; Boeck, T.; Lux-Steiner, M.C.; et al. Local Growth of CuInSe2 Micro Solar Cells for Concentrator Application. Mater. Today Energy 2017, 6, 238–247. [Google Scholar] [CrossRef]
  25. Correia, D.; Siopa, D.; Colombara, D.; Tombolato, S.; Salomé, P.M.P.; Abderrafi, K.; Anacleto, P.; Dale, P.J.; Sadewasser, S. Area-Selective Electrodeposition of Micro Islands for CuInSe2-Based Photovoltaics. Results Phys. 2019, 12, 2136–2140. [Google Scholar] [CrossRef]
  26. Siopa, D.; El Hajraoui, K.; Tombolato, S.; Babbe, F.; Lomuscio, A.; Wolter, M.H.; Anacleto, P.; Abderrafi, K.; Deepak, F.L.; Sadewasser, S.; et al. Micro-Sized Thin-Film Solar Cells via Area-Selective Electrochemical Deposition for Concentrator Photovoltaics Application. Sci. Rep. 2020, 10, 14763. [Google Scholar] [CrossRef]
  27. Fuster, D.; Anacleto, P.; Virtuoso, J.; Zutter, M.; Brito, D.; Alves, M.; Aparicio, L.; Fuertes Marrón, D.; Briones, F.; Sadewasser, S.; et al. System for Manufacturing Complete Cu(In,Ga)Se2 Solar Cells in Situ under Vacuum. Sol. Energy 2020, 198, 490–498. [Google Scholar] [CrossRef]
  28. Hu, D.; Ma, B.; Li, X.; Lv, Y.; Chen, Y.; Wang, C. Innovative and Sustainable Separation and Recovery of Valuable Metals in Spent CIGS Materials. J. Clean. Prod. 2022, 350, 131426. [Google Scholar] [CrossRef]
  29. Duchatelet, A.; Nguyen, K.; Grand, P.P.; Lincot, D.; Paire, M. Self-Aligned Growth of Thin Film Cu(In,Ga)Se2 Solar Cells on Various Micropatterns. Appl. Phys. Lett. 2016, 109, 253901. [Google Scholar] [CrossRef]
  30. Poeira, R.G.; Pérez-Rodríguez, A.; Prot, A.J.M.; Alves, M.; Dale, P.J.; Sadewasser, S. Direct Fabrication of Arrays of Cu(In,Ga)Se2 Micro Solar Cells by Sputtering for Micro-Concentrator Photovoltaics. Mater. Des. 2023, 225, 111597. [Google Scholar] [CrossRef]
  31. Ramanujam, J.; Singh, U.P. Copper Indium Gallium Selenide Based Solar Cells—A Review. Energy Environ. Sci. 2017, 10, 1306–1319. [Google Scholar] [CrossRef]
  32. Zaretskaya, E.P.; Gremenok, V.F.; Riede, V.; Schmitz, W.; Bente, K.; Zalesski, V.B.; Ermakov, O.V. Raman Spectroscopy of CuInSe2 Thin Films Prepared by Selenization. J. Phys. Chem. Solids 2003, 64, 1989–1993. [Google Scholar] [CrossRef]
  33. Choi, I.H. Raman Spectroscopy of CuIn1−XGaxSe2 for in-Situ Monitoring of the Composition Ratio. Thin Solid Films 2011, 519, 4390–4393. [Google Scholar] [CrossRef]
Figure 1. Schematic of the fabrication process of the pre-structured substrates.
Figure 1. Schematic of the fabrication process of the pre-structured substrates.
Nanomaterials 14 00543 g001
Figure 2. CAD design of the micro-dots pattern matrix. The rectangular shapes represent testing areas for thin film and/or device characterizations.
Figure 2. CAD design of the micro-dots pattern matrix. The rectangular shapes represent testing areas for thin film and/or device characterizations.
Nanomaterials 14 00543 g002
Figure 3. SLG–Mo–SiOx substrate mounted on standard Si wafer used for (a) photoresist coating and development; (b) SLG–Mo–SiOx substrate mounted next to a bare SLG substrate for RIE; (c) close-up of trapped air bubbles in the bare SLG substrate mounted with wax for RIE.
Figure 3. SLG–Mo–SiOx substrate mounted on standard Si wafer used for (a) photoresist coating and development; (b) SLG–Mo–SiOx substrate mounted next to a bare SLG substrate for RIE; (c) close-up of trapped air bubbles in the bare SLG substrate mounted with wax for RIE.
Nanomaterials 14 00543 g003
Figure 4. Heating profile for 2-stage selenization.
Figure 4. Heating profile for 2-stage selenization.
Nanomaterials 14 00543 g004
Figure 5. Optical images of micro-holes exposed with (a) DWL and (b) mask aligner. Micro-holes after (c) SiOx etching run (different colors indicate variations in the SiOx layer thickness) and (d) completely etched. SEM micrographs of micro-holes exposed with (e) DWL and (f) mask aligner after SiOx etching.
Figure 5. Optical images of micro-holes exposed with (a) DWL and (b) mask aligner. Micro-holes after (c) SiOx etching run (different colors indicate variations in the SiOx layer thickness) and (d) completely etched. SEM micrographs of micro-holes exposed with (e) DWL and (f) mask aligner after SiOx etching.
Nanomaterials 14 00543 g005
Figure 6. (a) Surface SEM micrograph of CIG precursor micro-dot before photoresist removal acquired at 20 kV; (bd) cross-sectional SEM micrographs of CIG micro-dot in the SiOx–photoresist matrix acquired at 5 kV. Colors were added in post-processing to improve clarity.
Figure 6. (a) Surface SEM micrograph of CIG precursor micro-dot before photoresist removal acquired at 20 kV; (bd) cross-sectional SEM micrographs of CIG micro-dot in the SiOx–photoresist matrix acquired at 5 kV. Colors were added in post-processing to improve clarity.
Nanomaterials 14 00543 g006
Figure 7. SEM micrographs of (a) as-deposited CIG and (b) after thermal annealing at 500 °C. Red squares highlight exposed Mo areas.
Figure 7. SEM micrographs of (a) as-deposited CIG and (b) after thermal annealing at 500 °C. Red squares highlight exposed Mo areas.
Nanomaterials 14 00543 g007
Figure 8. Top-view and up-close SEM micrographs of (ad) as-deposited CIG, (be) annealed at 500 °C, and (cf) selenized. SEM micrograph (f) acquired after CdS deposition. Red rectangles highlight cracking in the SiOx film.
Figure 8. Top-view and up-close SEM micrographs of (ad) as-deposited CIG, (be) annealed at 500 °C, and (cf) selenized. SEM micrograph (f) acquired after CdS deposition. Red rectangles highlight cracking in the SiOx film.
Nanomaterials 14 00543 g008
Figure 9. Raman spectrum of CIGS micro-absorber film after KCN (5%) etching and CdS deposition.
Figure 9. Raman spectrum of CIGS micro-absorber film after KCN (5%) etching and CdS deposition.
Nanomaterials 14 00543 g009
Table 1. Summary of top-down and bottom-up fabrication approaches of CIGS micro solar cells.
Table 1. Summary of top-down and bottom-up fabrication approaches of CIGS micro solar cells.
FabricationDeposition MethodMaterialSize of Micro
Solar Cell (µm)
Efficiency
under 1 Sun (%)
Efficiency under Concentration (%)Reference
Top-Down
Photolithography after bufferCo-evaporationCu(In,Ga)Se2151317 (×120)[19]
Photolithography after i-ZnOCo-evaporationCu(In,Ga)Se215~14~17[18]
25~11.5~16.5 (×120)
50~13~16.5
Photolithography after i-ZnOCo-evaporationCu(In,Ga)Se25016.321.3 (×475)[15]
Photolithography and chemical etchingCo-evaporationCu(In,Ga)Se240~13~17 (×100)[21]
250~11.5~15 (×40)
P1, P2, and P3 scribingCo-evaporationCu(In,Ga)Se21000 *13.515 (×6)[22]
500 *11.814.6 (×8)
750 (dot-shaped)13.617.6 (×51)
Bottom-Up
Patterned substratePVD CuInSe240–602.93.1 (×3)[24]
Laser-patterned substrateNucleation (PVD)CuInSe2
Cu(In,Ga)Se2
~4002.93.06 (×3)[23]
1.43.36 (×20)
Laser-patterned substrateLIFTCu(In,Ga)Se2~4900.150.237 (×20)[23]
Patterned substrateArea-selective
electrodeposition
CuInSe22004.8-[25]
Patterned substrateArea-selective
electrodeposition
Cu(In,Ga)Se22004.85.2 (×3)[26]
* lateral cell width.
Table 2. Elemental compositions of the as-deposited, annealed, and CIGS films.
Table 2. Elemental compositions of the as-deposited, annealed, and CIGS films.
SampleComposition (at %)Ratios
CuInGaSeCGIGGI
CIG46 ± 1.938 ± 1.813 ± 1.0-0.88 ± 0.040.26 ± 0.02
CIG50045 ± 1.739 ± 1.715 ± 1.8-0.84 ± 0.040.28 ± 0.03
CIGS24 ± 0.820 ± 1.55 ± 1.550 ± 0.91.00 ± 0.040.20 ± 0.06
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content.

Share and Cite

MDPI and ACS Style

Alves, M.; Anacleto, P.; Teixeira, V.; Carneiro, J.; Sadewasser, S. Fabrication of Pre-Structured Substrates and Growth of CIGS Micro-Absorbers. Nanomaterials 2024, 14, 543. https://0-doi-org.brum.beds.ac.uk/10.3390/nano14060543

AMA Style

Alves M, Anacleto P, Teixeira V, Carneiro J, Sadewasser S. Fabrication of Pre-Structured Substrates and Growth of CIGS Micro-Absorbers. Nanomaterials. 2024; 14(6):543. https://0-doi-org.brum.beds.ac.uk/10.3390/nano14060543

Chicago/Turabian Style

Alves, Marina, Pedro Anacleto, Vasco Teixeira, Joaquim Carneiro, and Sascha Sadewasser. 2024. "Fabrication of Pre-Structured Substrates and Growth of CIGS Micro-Absorbers" Nanomaterials 14, no. 6: 543. https://0-doi-org.brum.beds.ac.uk/10.3390/nano14060543

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop