Next Article in Journal
4H-SiC Schottky Barrier Diodes for Efficient Thermal Neutron Detection
Next Article in Special Issue
Study on Structural Design and Analysis of Composite Boat Hull Manufactured by Resin Infusion Simulation
Previous Article in Journal
Thermally Treated Waste Silt as Filler in Geopolymer Cement
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

Magnetic Properties of Novel Layered Disulfides CuCr0.99Ln0.01S2 (Ln = La…Lu)

by
Evgeniy V. Korotaev
*,
Mikhail M. Syrokvashin
,
Irina Yu. Filatova
and
Valentina V. Zvereva
Nikolaev Institute of Inorganic Chemistry, Siberian Branch of Russian Academy of Sciences, 630090 Novosibirsk, Russia
*
Author to whom correspondence should be addressed.
Submission received: 18 August 2021 / Revised: 1 September 2021 / Accepted: 3 September 2021 / Published: 6 September 2021

Abstract

:
The comprehensive study of the lanthanide-doped solid solutions CuCr0.99Ln0.01S2 (Ln = La…Lu) magnetic properties was carried out using static magnetochemistry and differential scanning calorimetry techniques. It was shown that magnetic properties of CuCr0.99Ln0.01S2 are significantly affected by the magnetic properties of the lanthanide ion. The magnetic susceptibility and the effective magnetic moment were found to deviate from the Curie-Weiss law in the temperature 90 K below and 50 K above the order-disorder transition at 695 K. The observed behavior of the temperature dependence of the effective magnetic moment in the order-disorder transition temperature region was described as a result of copper atoms redistribution over different types of the crystallographic sites.

1. Introduction

The main trends of modern material science are the improvement of existing and the development of new functional materials. Layered chromium dichalcogenides CrX2-based (X = S, Se, Te) compounds can be considered as promising functional materials. The unstable dichalcogenide CrX2-layers can be stabilized by the intercalation of electropositive metal atoms between the adjacent dichalcogenide layers [1,2]. The functional properties of the layered CrX2-based materials could be modified by the cationic substitution of chromium atoms in the dichalcogenide layers or by simultaneous intercalation of metal atoms of different types between CrX2-layers. For instance, in CuCrS2, the unstable CrS2-layers are stabilized by copper atoms. This results in the layered structure of CuCrS2 that is formed by the alternating copper and dichalcogenide layers. The CuCrS2-based solid solutions CuCr1-xMxS2 are promising functional materials with thermoelectric, superionic, and magnetic properties [3,4,5,6,7,8,9,10]. Chromium atoms could be substituted with other 3d-metal atoms over a wide concentration range (x ≤ 0.40) without changes in the crystal structure of the initial matrix [6,11,12]. The cationic substitution of CuCrS2-matrix with heavier 3d- or 4f-metal atoms allows one to decrease the thermal conductivity due to the phonon scattering increase [8,13,14]. The reported thermoelectric properties of CuCr1-xMxS2 allow one to consider these compounds for the fabrication of high-performance thermoelectric generators (TEGs) [7,8]. The redistribution of copper atoms over the different sites in CuCr1-xMxS2-structure allows one to consider CuCrS2-based solid solutions as promising materials for solid-state power sources, ion-selective membranes, and chemical sensors [6,15,16]. The magnetic properties of CuCrS2-based solid solutions can be used for the fabrication of spin gates, filters, and magnetic memory devices [5,17].
The magnetic properties of the initial CuCrS2-matrix are related to the ferromagnetic ordering of the magnetic moments of chromium atoms in CrS2-layers and to the antiferromagnetic ordering of the adjacent layers. The antiferromagnetic ordering in CuCrS2 could be observed at temperatures below the Neel temperature (TN ≈ 40 K). Above TN temperature, CuCrS2-matrix and CuCr1-xMxS2 solid solutions become paramagnetic and their magnetic susceptibility follows the Curie-Weiss law [2,8,17,18,19,20,21]. As was mentioned above, the phonon scattering has a significant impact on the thermoelectric properties of the material. The phonon scattering enhancement due to the presence of the atoms bearing magnetic moment improves the thermoelectric properties [22]. The cationic substitution of chromium by atoms with different magnetic moment values should significantly affect the phonon scattering efficiency. The magnetic moment of Ln ions is significantly changed across the lanthanide series. Thus, the magnetic properties of the lanthanide-doped CuCr1-xLnxS2 solid solutions are of special interest. As was previously reported, the optimal doping concentration for CuCrS2-based solid solutions is x = 0.01 [7,8]. An increase of x causes the Seebeck coefficient suppression due to the metal-insulator transition (MIT). Hence, here we report the study of magnetic properties of the lanthanide-doped CuCr0.99Ln0.01S2 (Ln = La…Lu) solid solutions.
CuCrS2-based materials exhibit a high-temperature order-disorder transition (ODT). The ODT affects the transport and thermoelectric properties in the high-temperature region (T > 670 K). As the temperature increases, the mobile metal atoms occupy sites that were unoccupied at room temperature. As a result, the electrical conductivity increases. The redistribution of the mobile metal atoms over crystallographic sites in CrS2-sublattice increases a structural disorder. The structural disorder reduces the lattice thermal conductivity resulting from the phonon scattering. Note that the ODT does not significantly affect the crystallographic structure of CuCrS2-matrix and has a reversible character. The magnetic susceptibility temperature dependence of CuCr1-xMxS2 follows the Curie-Weiss law in the temperature region above and below the ODT [2,19]:
χ T = C T θ = N A μ B 2 3 k T θ μ eff 2
where T is temperature, k is the Boltzmann constant, NA is the Avogadro number, μB is the Bohr magneton, μeff is the effective magnetic moment, and θ is Weiss constant:
θ = 2 j j + 1 3 k z i J i
where j is the total angular momentum quantum number, zi is the magnetic coordination number, Ji is the exchange interaction between magnetic centers, and i is the magnetic center number.
However, it should be noted that reported data do not include a detailed study of the magnetic properties in the ODT temperature region. The typical temperature resolution in the corresponding region exceeds 50 degrees [2,8,19]. Nevertheless, the physical properties of CuCrS2-matrix dramatically change in the immediate vicinity of the ODT (about ±50 degrees) [3]. Thus, the detailed study of the magnetic properties of CuCr0.99Ln0.01S2 in the immediate vicinity of the ODT is of special interest and has not been reported yet.
The synthesis procedure significantly affects the magnetic properties of CuCrS2-matrix. The different experimental works report on the contradictory results concerning the effective magnetic moment (µeff) and Weiss constant (θ) of CuCrS2. Thus, µeff and θ lie within the wide range of values 3.8 to 5.5 µB and −110 to −150 K, respectively. Furthermore, in case of the cation substituted solid solutions based on CuCrS2-matrix, the Weiss constant values are spread out even more [4,6,7,18,23]. For instance, some of the CuCrS2-based solid solutions were reported to have positive θ values [24]. This fact indicates the presence of a significant ferromagnetic contribution to the magnetic susceptibility value. It should be noted that the corresponding contribution could be due to the presence of specific ferromagnetic impurities [21]. Thus, in this study, the ferromagnetic contribution in the magnetic susceptibility value was taken into account.
Here, we report the study of the ODT and cationic substitution effect on the magnetic properties of lanthanide-doped CuCr0.99Ln0.01S2 (Ln = La … Lu) solid solutions using both differential scanning calorimetry (DSC) and static magnetochemistry techniques.

2. Experimental

The powder samples studied were synthesized from the initial metal oxides using a previously reported procedure [3,8]. The average grain size was 25 µm. The X-ray powder diffraction (XRD) experiment was carried out using non-monochromatic CuKα-radiation on a Shimadzu XRD 7000S diffractometer (Shimadzu Corporation, Kyoto, Japan). The XRD patterns were found quite similar. Figure 1 shows typical XRD patterns of the initial matrix and some solid solutions CuCr0.99Ln0.01S2. The XRD patterns of all CuCr0.99Ln0.01S2 (Ln = La…Lu) synthesized samples are shown in Supplementary Figure S1. The observed diffraction peaks on the XRD pattern indicate that the synthesized CuCrS2 sample has a rhombohedral structure with an R3m space group. The absence of the additional diffraction peaks allows one to conclude that synthesized samples are single-phase. The position and diffraction peaks intensity are in good agreement with the XRD data of the Inorganic Crystal Structure Database (database code 100594, denoted as “ICSD” in Figure 1) [25]. The calculated unit cell parameters a = 3.48(3) and c = 18.71(6) Å correlate well with the previously reported and reference data [7,25,26]. The lattice parameters of CuCr0.99Ln0.01S2 are close to those for CuCrS2-matrix and lies within the range of 3.47–3.48 and 18.67–18.71 Å for a and c, respectively. However, the unit cell volume slightly decreases due to the lanthanide contraction with an increase of the Ln atomic number (Supplementary Table S1 in Supplementary Materials). Thus, one can conclude that cationic substitution by lanthanides does not significantly affect the initial matrix crystal structure.
The elemental composition of the samples studied was controlled by X-ray fluorescence analysis using a Bruker MISTRAL M1 (Bruker Corporation, Billerica, MA, USA). The composition of the investigated solid solutions correlates well with the reference concentrations (Supplementary Table S2).
The magnetic properties of CuCr0.99Ln0.01S2 were measured using the Faraday method in the wide temperature range of 80–750 K. The temperature stabilization was controlled using a Delta DTB9696 temperature controller (Delta Electronics, Taipei, Taiwan). The voltage from a quartz torque microbalance was measured using Keysight 34465 A digital voltmeter (Keysight Technologies, Santa-Rosa, CA, USA). The magnetic field strength was varied in the range of 4.8 to 8.6 kOe. The magnetic field strength fluctuations did not exceed 2%. The powder samples (~20 mg) were placed in open quartz ampoules and vacuumed at 0.01 Torr pressure. During the measurements, the samples were held in a helium atmosphere at 5 Torr pressure. The diamagnetic contributions into the magnetic susceptibility value were taken into account using the Pascal scheme. The field dependence of the magnetic susceptibility χ(1/H) was measured in order to take into account the possible presence of the ferromagnetic contribution to the magnetic susceptibility value. The effective magnetic moment as a function of temperature was calculated as follows [21,27]:
μ eff T = 8 χ T
The thermal effects accompanying the ODT phase transition were studied using a DSC-500 differential scanning calorimeter (LLC Specpribor, Samara, Russia). The powder samples (~15 mg) were placed in open aluminum crucibles. The DSC signals were measured in the argon flow (50 mL/min) at a constant heating rate of 10 °C/min.

3. Results and Discussion

Magnetic susceptibility (χ) of chemical compounds is the sum of the different magnetic contributions (paramagnetic, ferromagnetic, and diamagnetic). The diamagnetic contributions are caused by the circulation of the electrons induced by an external magnetic field. The paramagnetic contribution is due to the presence of the unpaired electrons in the material and the field-induced electronic transitions (Van Vleck paramagnetism). The ferromagnetic impurities could significantly affect the magnetic susceptibility value (ferromagnetic contributions). These contributions can be taken into account using the magnetic susceptibility values measured at few different magnetic fields (H). The positive slope of χ(1/H) indicates the ferromagnetic contribution in the measured magnetic susceptibility value. The χ(1/H) behavior of the solid solutions studied were found quite similar. The typical χ(1/H) dependencies are shown in Figure 2. The zero slope of χ(1/H) indicates that the significant ferromagnetic contribution in χ is absent. Thus, one can conclude that the samples studied have no ferromagnetic impurities.
The behavior of the measured molar magnetic susceptibility temperature dependencies of CuCr0.99Ln0.01S2 was found quite similar. The typical dependencies of χ(T), 1/χ(T), μeff(T) of CuCrS2 and several lanthanide-doped solid solutions CuCr0.99Ln0.01S2 (Ln = La, Nd, Gd, Dy, Er, Lu) are shown in Figure 3. The Curie-Weiss law (Equation (1)) was used to calculate the effective magnetic moment (μeff) and the Weiss constant (θ) values. The μeff value of 3.77 μB for CuCrS2 was in a good agreement with the experimental data reported previously and corresponded to the theoretical value for Cr3+ state (μeff (Cr3+) = 3.87 μB). Note that for CuCrS2 experimental μeff value, it lay within the range of 3.75–3.79 μB [5,20,21,26,27]. The Weiss constant of −140 K correlates well with the reported data and lies within the range of −110 to −150 K [5,20,21,23,27].
The calculated values of μeff and θ for the entire series of the samples studied are plotted in Figure 4a,b. The calculated μeff(Z) and θ(Z) have a non-monotonic behavior (Z is the lanthanide atomic number). The maximal μeff value was observed for CuCr0.99Dy0.01S2, the minimal one for CuCr0.99La0.01S2. Note that in the lanthanide series, the dysprosium and lanthanum atoms have the maximal and the minimal theoretical μeff value of 10.6 and 0.0 µB, respectively [27,28,29]. Thus, one can conclude that observed μeff(Z) behavior is associated with the lanthanide magnetic moment. Taking into account the isovalent cationic substitution character in CuCr0.99Ln0.01S2 (Ln = La, Ce) solid solutions [8,30], the theoretical μeff(Z) could be calculated (Figure 4c). The theoretical μeff(Z) for CuCr0.99Ln0.01S2 solid solutions were calculated using table μeff values of Ln3+ ions and experimental μeff value of CuCrS2-matrix [27,29]. The obtained experimental μeff(Z) correlates well with the theoretical data calculated using non-interacting spin approximation (Figure 3a,c).
The Weiss constant is related to the exchange interaction between paramagnetic centers. In contrast to CuCrS2-matrix, the magnetic properties of CuCr0.99Ln0.01S2 are determined not only by the magnetic Cr3+ ions, but also by Ln3+ lanthanide ions contributions. Thus, the observed non-linear behavior of θ as a function of Z is determined by the lanthanide contribution. In terms of molecular field theory, the Weiss constant is proportional to the spin (for 3d-metals) or to the total angular momentum quantum number j (for lanthanides). Hence, the theoretical j(Z) dependence for lanthanide ions was plotted in Figure 4d. Note that both j(Z) and θ(Z) dependencies have a similar behavior (Figure 4b,d). The minimal θ values are attributed to the solid solutions doped with lanthanum, europium, and lutetium. This is due to the fact that 4f-orbital is either empty (La) or completely filled (Lu), where j = 0. The observed Weiss constant decrease for CuCr0.99Eu0.01S2 solid solution is due to the spin and orbital magnetic moments compensation (spin-orbit compensation) [31]. Thus, the zero value of j leads to the absence of the contribution of the lanthanide atoms to the exchange interaction integrals in Equation (2). The decrease of the θ absolute value indicates the weakening of the antiferromagnetic interactions after the cationic substitution of chromium with lanthanide atoms with j ≠ 0.
Thus, the behavior of the magnetic properties of the lanthanide-doped solid solutions CuCr0.99Ln0.01S2 (Ln = La…Lu) is majorly determined by the lanthanide ion magnetic properties. Thereby, the most significant effect was observed for lanthanides with the highest j (from Tb to Er).
As was discussed above, the magnetic properties of CuCr1-xLnxS2 in the ODT temperature region are of special interest. The magnetic susceptibility of the initial copper-chromium disulfide and CuCrS2-based solid solutions in the temperature region of 100 to 800 K is commonly described in terms of the Curie-Weiss law [2,6,20]. However, the improving of the temperature resolution from ~50 K to 10 K allows one to observe the deviation from the Curie–Weiss law in the ODT temperature region (Figure 3a). The corresponding effect could be clearly observed in the effective magnetic moment temperature dependencies μeff(T) (Figure 3c). For clarity, the enlarged curves of μeff(T) within the temperature range ~90 K below and ~50 K above the ODT (TODT~695 K) are plotted in Figure 3d. The corresponding temperature region exhibits an inflection feature. This fact allows one to conclude that the μeff value is affected by the ODT. As it was reported previously, the ODT in CuCrS2 and similar layered dichalcogenides could be studied using DSC technique [3,13,32]. In this regard, the DSC signals of CuCr0.99Ln0.01S2 were measured in the same temperature region (Figure 5). The measured DSC signals exhibit a single peak at ~694–695 K. Thus, the position of the inflection feature on μeff(T) dependencies and peak on the DSC curves are correlated well. At room temperature, copper atoms are localized at the “ordered” tetrahedral sites between CrS2-layers, whereas the “disordered” octahedral sites remain unoccupied [10,26,33,34]. With the temperature increase, the occupation probability of octahedral sites increases. Hence, in the temperature region above the ODT, copper atoms are statistically distributed between tetrahedral and octahedral sites. The “ordered” tetrahedral sites were shifted to CrS2-layer, whereas octahedral sites were centered between two adjacent CrS2-layers. Since μeff(T) decreases at T < TODT, one can conclude that copper atoms in octahedral sites provide more efficient channels for the indirect exchange interaction than atoms in tetrahedral sites. The exchange interaction increase resulted in an increase in the Weiss constant (see Equation (2)). The further temperature increase lead to μeff(T) an increase at T > TODT due to the magnetic moments disordering of Cr and Ln ions. Thus, the observed μeff(T) behavior could be associated with the redistribution of the copper atoms over different crystallographic sites caused by the ODT.

4. Conclusions

A comprehensive study of CuCr0.99Ln0.01S2 (Ln = La…Lu) magnetic properties in a wide temperature range of 80–740 K was carried out. It was established that the effective magnetic moment and the Weiss constant of the lanthanide-doped solid solutions are significantly affected by the total angular momentum quantum number j and the effective magnetic moment of the lanthanide ion. The most significant effect on the magnetic properties was observed for solid solutions doped with Tb, Dy, Ho, and Er. Thus, these lanthanides are the most promising candidates for the modification of CuCrS2-based solid solutions magnetic properties. The magnetic properties’ behavior in the immediate vicinity of the ODT was reported for the first time. The magnetic susceptibility and the effective magnetic moment of CuCr0.99Ln0.01S2 were found to decrease at temperatures below the ODT. The observed behavior of the effective magnetic moment temperature dependence in the ODT temperature region was described as a result of copper atoms redistribution over different types of crystallographic sites.

Supplementary Materials

The following are available online at https://0-www-mdpi-com.brum.beds.ac.uk/article/10.3390/ma14175101/s1, Figure S1: Powder diffraction patterns of CuCrS2-matrix and CuCr0.99Ln0.01S2 solid solutions, Table S1: Lattice parameters of CuCr0.99Ln0.01S2, Table S2: Elemental composition of CuCr0.99Ln0.01S2.

Author Contributions

Conceptualization, E.V.K. and M.M.S.; methodology, E.V.K.; investigation, E.V.K., M.M.S. and V.V.Z.; synthesis, I.Y.F.; writing—original draft preparation, E.V.K. and M.M.S.; writing—review and editing, E.V.K. and M.M.S.; visualization, E.V.K. and M.M.S.; supervision, E.V.K.; project administration, E.V.K.; funding acquisition, E.V.K. All authors have read and agreed to the published version of the manuscript.

Funding

This study was funded by the Russian Science Foundation (project No. 19-73-10073).

Institutional Review Board Statement

Not applicable.

Informed Consent Statement

Not applicable.

Data Availability Statement

The data presented in this study are available in Supplementary Materials.

Acknowledgments

E.V. Korotaev, M.M. Syrokvashin, and I.Yu. Filatova appreciate the Russian Science Foundation for their support. V.V. Zvereva appreciates the Ministry of Science and Higher Education of the Russian Federation (No. 121031700313-8).

Conflicts of Interest

The authors declare that they have no conflict of interest.

References

  1. Engelsman, F.M.R.; Wiegers, G.A.; Jellinek, F.; Van Laar, B. Crystal structures and magnetic structures of some metal(I) chromium(III) sulfides and selenides. J. Solid State Chem. 1973, 6, 574–582. [Google Scholar] [CrossRef]
  2. Bongers, P.F.; Van Bruggen, C.F.; Koopstra, J.; Omloo, W.P.F.A.M.; Wiegers, G.A.; Jellinek, F. Structures and magnetic properties of some metal (I) chromium (III) sulfides and selenides. J. Phys. Chem. Solids 1968, 29, 977–984. [Google Scholar] [CrossRef]
  3. Korotaev, E.V.; Syrokvashin, M.M.; Filatova, I.Y.; Sotnikov, A.V. Effect of the Order-Disorder Transition on the Electronic Structure and Physical Properties of Layered CuCrS2. Materials 2021, 14, 2729. [Google Scholar] [CrossRef]
  4. Rasch, J.C.E.; Boehm, M.; Ritter, C.; Mutka, H.; Schefer, J.; Keller, L.; Abramova, G.M.; Cervellino, A.; Löffler, J.F. Magnetoelastic coupling in the triangular lattice antiferromagnet CuCrS2. Appl. Phys. Lett. 2009, 80, 104431. [Google Scholar]
  5. Karmakar, A.; Dey, K.; Chatterjee, S.; Majumdar, S.; Giri, S. Spin correlated dielectric memory and rejuvenation in multiferroic CuCrS2. Appl. Phys. Lett. 2014, 104, 052906. [Google Scholar] [CrossRef] [Green Version]
  6. Almukhametov, R.F.; Yakshibayev, R.A.; Gabitov, E.V.; Abdullin, A.R.; Kutusheva, R.M. Structural properties and ionic conductivities of CuCr1–xVxS2 solid solutions. Phys. Status Solidi 2003, 236, 29–33. [Google Scholar] [CrossRef]
  7. Korotaev, E.V.; Syrokvashin, M.M.; Filatova, I.Y.; Pelmenev, K.G.; Zvereva, V.V.; Peregudova, N.N. Seebeck Coefficient of Cation-Substituted Disulfides CuCr1−xFexS2 and Cu1−xFexCrS2. J. Electron. Mater. 2018, 47, 3392–3397. [Google Scholar] [CrossRef]
  8. Korotaev, E.V.; Syrokvashin, M.M.; Filatova, I.Y.; Trubina, S.V.; Nikolenko, A.D.; Ivlyushkin, D.V.; Zavertkin, P.S.; Sotnikov, A.V.; Kriventsov, V.V. XANES investigation of novel lanthanide-doped CuCr0.99Ln0.01S2 (Ln = La, Ce) solid solutions. Appl. Phys. A 2020, 126, 537. [Google Scholar] [CrossRef]
  9. Hansen, A.-L.; Dankwort, T.; Groß, H.; Etter, M.; König, J.; Duppel, V.; Kienle, L.; Bensch, W. Structural properties of the thermoelectric material CuCrS2 and of deintercalated CuxCrS2 on different length scales: X-ray diffraction, pair distribution function and transmission electron microscopy studies. J. Mater. Chem. C 2017, 5, 9331–9338. [Google Scholar] [CrossRef]
  10. Al’mukhametov, R.F.; Yakshibaev, R.A.; Gabitov, É.V.; Abdullin, A.R. Investigation of superionic phase transition in the CuCr1-xVxS2 system by X-ray diffraction and magnetic methods. Phys. Solid State 2000, 42, 1508–1511. [Google Scholar] [CrossRef]
  11. Tsujii, N.; Kitazawa, H.; Kido, G. Insulator to metal transition induced by substitution in the nearly two-dimensional compound CuCr1-xVxS2. Phys. Status Solidi Curr. Top. Solid State Phys. 2006, 3, 2775–2778. [Google Scholar]
  12. Al’mukhametov, R.F.; Yakshibaev, R.A.; Gabitov, E.V.; Abdullin, A.R. Synthesis and X-ray diffraction study of CuCr1-xVxS2. Inorg. Mater. 2000, 36, 437–440. [Google Scholar] [CrossRef]
  13. Wu, D.; Huang, S.; Feng, D.; Li, B.; Chen, Y.; Zhang, J.; He, J. Revisiting AgCrSe2 as a promising thermoelectric material. Phys. Chem. Chem. Phys. 2016, 18, 23872–23878. [Google Scholar] [CrossRef]
  14. Bhattacharya, S.; Basu, R.; Bhatt, R.; Pitale, S.; Singh, A.; Aswal, D.K.; Gupta, S.K.; Navaneethan, M.; Hayakawa, Y. CuCrSe2: A high performance phonon glass and electron crystal thermoelectric material. J. Mater. Chem. A 2013, 1, 11289–11294. [Google Scholar] [CrossRef]
  15. Guy, D.R.P.; Marseglia, E.A.; Guy, S.C. Electron Spin Resonance in CuCrS2 and CuCrSe2 Single Crystals. Mol. Cryst. Liq. Cryst. 1985, 121, 165–168. [Google Scholar] [CrossRef]
  16. Akmanova, G.R.; Davletshina, A.D. Ionic conductivity and diffusion in superionic conductors CuCrS2-AgCrS2. Lett. Mater. 2013, 3, 76–78. [Google Scholar] [CrossRef] [Green Version]
  17. Abramova, G.M.; Petrakovskii, G.A. Metal-insulator transition, magnetoresistance, and magnetic properties of 3d-sulfides (Review). Low Temp. Phys. 2006, 32, 725–734. [Google Scholar] [CrossRef]
  18. Tsujii, N.; Kitazawa, H. Substitution effect on the two-dimensional triangular-lattice system CuCrS2. J. Phys. Condens. Matter 2007, 19, 145245. [Google Scholar] [CrossRef]
  19. Al’mukhametov, R.F.; Yakshibaev, R.A.; Gabitov, É.V. Magnetic and transport properties of CuCr1−xVxS2 compounds. Phys. Solid State 1999, 41, 1327–1328. [Google Scholar] [CrossRef]
  20. Vasilyeva, I.G. Chemical aspect of the structural disorder in CuCrS2 and CuCr1–xVxS2 solid solutions. J. Struct. Chem. 2017, 58, 1009–1017. [Google Scholar] [CrossRef]
  21. Korotaev, E.V.; Syrokvashin, M.M.; Filatova, I.Y.; Zvereva, V.V. Vanadium doped layered copper-chromium sulfides: The correlation between the magnetic properties and XES data. Vacuum 2020, 179, 109390. [Google Scholar] [CrossRef]
  22. Zhang, J.Y.; Zhu, J.H.; You, L.; Guo, K.; Li, Z.L.; Lin, W.G.; Huang, J.; Luo, J. Enhanced and stabilized n-type thermoelectric performance in α-CuAgSe by Ni doping. Mater. Today Phys. 2019, 10, 100095. [Google Scholar] [CrossRef]
  23. Tewari, G.C.; Tripathi, T.S.; Rastogi, A.K. Thermoelectric properties of layer-antiferromagnet CuCrS2. J. Electron. Mater. 2010, 39, 1133–1139. [Google Scholar] [CrossRef] [Green Version]
  24. Abramova, G.M.; Petrakovskǐ, G.A.; Vorotynov, A.M.; Velikanov, D.A.; Kiselev, N.I.; Bovina, A.F.; Szymczak, R.; Al’mukhametov, R.F. Phase transitions and colossal magnetoresistance in CuVxCr1−xS2 layered disulfides. JETP Lett. 2006, 83, 118–121. [Google Scholar] [CrossRef]
  25. Inorganic Crystal Structure Database, Version 2.1.0. Leibniz Institute for Information Infrastructure, FIZ Karlsruhe, Eggenstein- Leopoldshafen, Germany, (n.d.). Available online: https://icsd.products.fiz-karlsruhe.de/ (accessed on 17 August 2021).
  26. Vassilieva, I.G.; Kardash, T.Y.; Malakhov, V.V. Phase transformations of CuCrS2: Structural and chemical study. J. Struct. Chem. 2009, 50, 288–295. [Google Scholar] [CrossRef]
  27. Selwood, P. Magnetochemistry, 2nd ed.; Interscience Publishers: New York, NY, USA, 1956. [Google Scholar]
  28. Le Nagard, N.; Collin, G.; Gorochov, O. Etude structurale et proprietes physiques de CuCrS2. Mater. Res. Bull. 1979, 14, 1411–1417. [Google Scholar] [CrossRef]
  29. Moeller, T. The Chemistry of the Lanthanides; Elsevier: Amsterdam, The Netherlands, 1973. [Google Scholar]
  30. Korotaev, E.V.; Syrokvashin, M.M.; Filatova, I.Y.; Trubina, S.V.; Nikolenko, A.D.; Ivlyushkin, D.V.; Zavertkin, P.S.; Kriventsov, V.V. The conduction band of the lanthanide doped chromium disulfides CuCr0.99Ln0.01S2 (Ln=La, Ce, Gd): XANES investigations. In Proceedings of the AIP Conference, Novosibirsk, Russian, 13–16 July 2020; Volume 2299, p. 080004. [Google Scholar]
  31. Adachi, H.; Ino, H. A ferromagnet having no net magnetic moment. Nature 1999, 401, 148–150. [Google Scholar] [CrossRef]
  32. Murphy, D.W.; Chen, H.S.; Tell, B. Superionic Conduction in AgCrS2 and AgCrSe2. J. Electrochem. Soc. 1977, 124, 1268–1271. [Google Scholar] [CrossRef]
  33. Korotaev, E.V.; Syrokvashin, M.M.; Peregudova, N.N.; Kanazhevskii, V.V.; Mazalov, L.N.; Sokolov, V.V. Effects of the nearest-neighbor environment of copper atoms on the XANES spectra of layered chromium-copper disulfides. J. Struct. Chem. 2015, 56, 596–600. [Google Scholar] [CrossRef]
  34. Korotaev, E.V.; Kanazhevskiy, V.V.; Peregudova, N.N.; Syrokvashin, M.M.; Mazalov, L.N.; Sokolov, V.V.; Filatova, I.Y.; Pichugin, A.Y. Xanes of X-ray absorbtion K edges of chromium dichalcogenides CuCr1-x M′xS2 and MCrX2. J. Struct. Chem. 2016, 57, 1355–1361. [Google Scholar] [CrossRef]
Figure 1. Powder diffraction patterns of CuCrS2-matrix and CuCr0.99Ln0.01S2 solid solutions (Ln = La, Gd, Ho).
Figure 1. Powder diffraction patterns of CuCrS2-matrix and CuCr0.99Ln0.01S2 solid solutions (Ln = La, Gd, Ho).
Materials 14 05101 g001
Figure 2. Magnetic susceptibility field dependencies χ(1/H) at T = 300 K: CuCrS2 (a), CuCr0.99Dy0.01S2(b).
Figure 2. Magnetic susceptibility field dependencies χ(1/H) at T = 300 K: CuCrS2 (a), CuCr0.99Dy0.01S2(b).
Materials 14 05101 g002
Figure 3. Molar magnetic susceptibility (a), inverse magnetic susceptibility (b), and effective magnetic moment (c,d), temperature dependencies. Solid lines are Curie-Weiss law approximation.
Figure 3. Molar magnetic susceptibility (a), inverse magnetic susceptibility (b), and effective magnetic moment (c,d), temperature dependencies. Solid lines are Curie-Weiss law approximation.
Materials 14 05101 g003
Figure 4. Experimental magnetic moment (a), Weiss constant (b), theoretical estimation of μeff (c), and the total angular momentum quantum number (d) as a function of lanthanide atomic number.
Figure 4. Experimental magnetic moment (a), Weiss constant (b), theoretical estimation of μeff (c), and the total angular momentum quantum number (d) as a function of lanthanide atomic number.
Materials 14 05101 g004
Figure 5. DSC-signal of initial CuCrS2-matrix and CuCr0.99Ln0.01S2 (Ln = La, Nd, Eu, Dy, Tm, Lu) solid solutions in the temperature region of the ODT.
Figure 5. DSC-signal of initial CuCrS2-matrix and CuCr0.99Ln0.01S2 (Ln = La, Nd, Eu, Dy, Tm, Lu) solid solutions in the temperature region of the ODT.
Materials 14 05101 g005
Publisher’s Note: MDPI stays neutral with regard to jurisdictional claims in published maps and institutional affiliations.

Share and Cite

MDPI and ACS Style

Korotaev, E.V.; Syrokvashin, M.M.; Filatova, I.Y.; Zvereva, V.V. Magnetic Properties of Novel Layered Disulfides CuCr0.99Ln0.01S2 (Ln = La…Lu). Materials 2021, 14, 5101. https://0-doi-org.brum.beds.ac.uk/10.3390/ma14175101

AMA Style

Korotaev EV, Syrokvashin MM, Filatova IY, Zvereva VV. Magnetic Properties of Novel Layered Disulfides CuCr0.99Ln0.01S2 (Ln = La…Lu). Materials. 2021; 14(17):5101. https://0-doi-org.brum.beds.ac.uk/10.3390/ma14175101

Chicago/Turabian Style

Korotaev, Evgeniy V., Mikhail M. Syrokvashin, Irina Yu. Filatova, and Valentina V. Zvereva. 2021. "Magnetic Properties of Novel Layered Disulfides CuCr0.99Ln0.01S2 (Ln = La…Lu)" Materials 14, no. 17: 5101. https://0-doi-org.brum.beds.ac.uk/10.3390/ma14175101

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop